Solstice

Solstice Advanced Materials Thermal Interface Materials & Heat Spreaders
Solstice Advanced Materials develops thermal-management materials for semiconductor packaging and electronic assemblies, including phase change materials, thermal gap pads, hybrid thermal materials, thermal greases, thermal insulators, putty pads, and heat spreaders. The business became an independent company in 2025 following the spin-off of Honeywell Advanced Materials, so some established product families and legacy product codes may still reflect their Honeywell origin.
Krayden supplies a selection of Solstice thermal-management materials and can support product comparison, interface and gap requirements, material-format selection, assembly considerations, and processing needs. Product suitability depends on the specific device architecture, thermal target, mechanical constraints, electrical-isolation requirements, and service environment.
Markets Served by Solstice Advanced Materials
Thermal Interface Materials
Solstice thermal interface materials are used between heat-generating components and heat-spreading or heat-removal surfaces to reduce air gaps and improve thermal contact. The portfolio spans thin-interface phase change materials, compressible gap pads, dispensable one- and two-part hybrid thermal materials, conformable putty pads, thermal greases, and electrically insulating thermal pads. Selection depends on interface geometry, bond-line or gap requirements, compressibility, electrical isolation, application method, rework needs, and the thermal and mechanical demands of the assembly.
Additional Solstice TIM families provide options for conformable putty-pad formats, pre-cured dispensable materials, grease interfaces, and electrically insulating thermal paths.
Heat Spreaders
Solstice heat spreaders are metal lid and heat-spreading components used in semiconductor thermal-management assemblies to distribute heat from the package toward a larger cooling interface. The appropriate manufacturing route depends on the required geometry, dimensions, material and plating requirements, package architecture, tooling approach, and expected production method.
Talk to our Experts
Krayden can help compare Solstice thermal interface materials and heat-spreader options for semiconductor, electronics, automotive, telecommunications, and high-performance-computing applications. Our team can support material selection, interface and gap requirements, electrical-isolation needs, application methods, processing considerations, and comparison of candidate thermal-management materials for your assembly.
Solstice Advanced Materials Quick Reference
64 products
-
TIP 1500 | Thermal insulator pad
- 0.54 - 0.61 Thermal Impedance
- 1.5 Thermal Conductivity
- 0.23mm Thickness
-
TIP 3500 | Thermal insulator pad
- 0.18 - 0.23 Thermal Impedance
- 3.5 Thermal Conductivity
- 0.25 - 0.50 mm Thickness
-
HT 3500 | One part Hybrid Thermal Gel
- Dark Red
- 3.5 Thermal Conductivity
- High flow rate
-
HLT 2000 | Two part Hybrid Thermal Gel
- Yellow + White
- 2.0 Thermal Conductivity
- Cost Effectiveness
-
TG 2000I | Thermal Grease
- 0.02 Thermal Impedance
- 2.0 Thermal Conductivity
- 30μm BLT
-
LTM 6300-SP | Phase Change Paste
- 0.12 - 0.14 Thermal Impedance
- 1.8 - 2.4 Thermal Conductivity
- Highest volume resistivity
-
TIP 5000 | Thermal insulator pad
- 0.15 - 0.18 Thermal Impedance
- 5.0 Thermal Conductivity
- 0.25 - 0.50 mm Thickness
-
HW-HSPS | Heat Spreader - Progressive Stamping
- Nickel plated / Au Spot
- Small and medium form factors
- Simplified parts - Lower volumes
-
HW-HSTD | Heat Spreader - Transfer die stamping
- Nickel plated / Au Spot
- Wide range form factor
- Complex designs - Higher volumes
-
HGP12 | High Thermal Conductivity Gap Pad
- 0.13 Thermal Impedance
- 12 Thermal Conductivity
- Low oil bleeding & Low volatile
-
HGP12PT | High Thermal Conductivity Putty Pad
- 0.13 Thermal Impedance
- 12 Thermal Conductivity
- Low oil bleeding & Low volatile
-
PCM 45F | Phase Change Pad
- 0.09 - 0.12 Thermal Impedance
- 2.0 - 2.5 Thermal Conductivity
- Pad form
-
TG1500I | Thermal Grease
- 0.03 Thermal Impedance
- 1.5 Thermal Conductivity
- 30μm BLT
-
HGPA12 | High Thermal Conductivity Gap Pad
- 0.14 Thermal Impedance
- 12 Thermal Conductivity
- Low oil bleeding & Low volatile
-
PCM 45F-SP | Phase Change Paste
- 0.09 - 0.12 Thermal Impedance
- 2.0 - 2.5 Thermal Conductivity
- High volume resistivity
-
HLT 1800 | Two part Hybrid Thermal Gel
- Yellow + White
- 1.8 Thermal Conductivity
- Cost effective
-
HGP14 | High Thermal Conductivity Gap Pad
- 0.10 Thermal Impedance
- 14 Thermal Conductivity
- Low oil bleeding & Low volatile
-
TG3010I | Thermal Grease
- 0.003 °C•cm²/W Thermal Impedance
- 3.0 W/m•K Thermal Conductivity
- 10μm BLT
-
TGP 1200 | Thermal Gap Pad
- 1.03 Thermal Impedance
- 1.2 Thermal Conductivity
- Competitive cost of ownership
-
TG 2800I | Thermal Grease
- 0.009 Thermal Impedance
- 2.8 Thermal Conductivity
- 25μm BLT
-
HT 4500 | One part Hybrid Thermal Gel
- Green
- 4.5 Thermal Conductivity
- Printable
-
HLP 2000 | Two part Thermal potting material
- Low Viscosity
- 2.0 Thermal Conductivity
- Room temperature cure
-
PTM 5000 | Phase Change Pad
- 0.06 - 0.08 Thermal Impedance
- 3.5 - 4.5 Thermal Conductivity
- Pad form
-
HT 5010 | One part Hybrid Thermal Gel
- Gray
- 5.2 Thermal Conductivity
- Best performing mid range TIM
-
TGP 1500 | Thermal Gap Pad
- 0.94 Thermal Impedance
- 1.5 Thermal Conductivity
- 0.5 - 5 mm Thickness
-
HLT 2000LV | Two part Hybrid Thermal Gel
- White + Dark Red
- 2.0 Thermal Conductivity
- Low volatility
-
TG 3000 | Thermal Grease
- 0.009 Thermal Impedance
- 3.0 Thermal Conductivity
- 25μm BLT
-
PTM 5000-SP | Phase Change Paste
- 0.06 - 0.08 Thermal Impedance
- 3.5 - 4.5 Thermal Conductivity
- Stencil Printable
-
TG 3000I | Thermal Grease
- 0.003 Thermal Impedance
- 3.0 Thermal Conductivity
- 7μm BLT
-
HT 7000 | One part Hybrid Thermal Gel
- Dark Red
- 7 Thermal Conductivity
- Horizontal mounting
-
HLT 3000 | Two part Hybrid Thermal Gel
- Blue + White
- 3.0 Thermal Conductivity
- Stencil Printable
-
TGP 2000E | Thermal Gap Pad
- 0.95 Thermal Impedance
- 2.0 Thermal Conductivity
- Excellent surface wetting
-
PTM 6000 | Phase Change Pad
- Higher reliability than PTM5000
- 3.5 - 4.5 Thermal Conductivity
- Pad form
-
TGP 3000 | Thermal Gap Pad
- 0.65 Thermal Impedance
- 3.0 Thermal Conductivity
- Low pressure versus deflection
-
HLT 3500 | Two part Hybrid Thermal Gel
- Blue + White
- 3.5 Thermal Conductivity
- 0.44 Thermal impedance
-
TG 4000 | Thermal Grease
- 0.005 Thermal Impedance
- 4.0 Thermal Conductivity
- 23μm BLT
-
HT 9000 | One part Hybrid Thermal Gel
- Dark Blue
- 9 Thermal Conductivity
- Silicon based
-
TG 5500 | Thermal Grease
- 0.01 Thermal Impedance
- 5.5 Thermal Conductivity
- 23μm BLT
-
HT 10000-R | One part Hybrid Thermal Gel
- Dark Gray
- 10 Thermal Conductivity
- Good dispense rate
-
HLT 3500LV | Two part Hybrid Thermal Gel
- Blue + White
- 3.5 Thermal Conductivity
- 0.44 Thermal impedance
-
TGP3000E | Thermal Gap Pad
- 0.65 Thermal Impedance
- 3.0 Thermal Conductivity
- Excellent surface wetting
-
PTM 6000HV | Phase Change Paste
- 0.14 Thermal Impedance
- 5.2 Thermal Conductivity
- Optimized for IGBT
-
HLT 7000 | Two part Hybrid Thermal Gel
- Dark Red + Gray
- 7.0 Thermal Conductivity
- High reliability
-
HT 11000 | One part Hybrid Thermal Gel
- Dark Gray
- 11 Thermal Conductivity
- Highest thermal conductivity
-
PTM6880 | Phase Change Pad
- 6,0 W/m•K thermal conductivity
- 0.056 ℃•cm²/W
- Improved flowability
-
PTM 7000 | Phase Change Pad
- 0.06 Thermal Impedance
- 6.5 Thermal Conductivity
- Pad form
-
HLT 10000 | Two part Hybrid Thermal Gel
- Dark Gray + Gray
- 10 Thermal Conductivity
- The pinnacle of TIM
-
TGP 3510PT | Thermal Putty Pad
- 0.45 Thermal Impedance
- 3.5 Thermal Conductivity
- 0.5 - 5 mm Thickness
-
PTM 7000-SP | Phase Change Paste
- 0.06 Thermal Impedance
- 6.5 Thermal Conductivity
- Paste form
-
TGP 5000 | Thermal Gap Pad
- 0.3 Thermal Impedance
- 5.0 Thermal Conductivity
- Good elastic modulus
-
PTM 7000-SPM | Phase Change Paste
- 0.06 Thermal Impedance
- 6.5 Thermal Conductivity
- Medium drying solvent
-
PTM 7900 | Phase Change Pad
- 0.045 Thermal Impedance
- 8.0 Thermal Conductivity
- Pad form
-
TGP 6000 | Thermal Gap Pad
- 0.25 Thermal Impedance
- 6.0 Thermal Conductivity
- Excellent surface wetting
-
PTM 7900-SP | Phase Change Paste
- 0.045 Thermal Impedance
- 8.0 Thermal Conductivity
- Paste form
-
-
TGP 6000PT | Thermal Putty Pad
- 0.27 Thermal Impedance
- 6.0 Thermal Conductivity
- 0.5 - 5 mm Thickness
-
PTM 7950-SP | Phase Change Paste
- 0.04 Thermal Impedance
- 8.5 Thermal Conductivity
- Paste form
-
PTM 7950-SPS | Phase Change Paste
- 0.04 Thermal Impedance
- 8.5 Thermal Conductivity
- Slow drying solvent
-
TGP 7500C | Thermal Gap Pad
- 0.16 Thermal Impedance
- 7.5 Thermal Conductivity
- Excellent surface wetting
-
TGP 8000 | Thermal Gap Pad
- 0.2 Thermal Impedance
- 8.0 Thermal Conductivity
- Low oil bleeding/Outgassing
-
TGP 8000PT | Thermal Putty Pad
- 0.19 Thermal Impedance
- 8.0 Thermal Conductivity
- 0.5 - 5 mm Thickness
-
TGP 8000HV | Thermal Gap Pad
- 0.2 Thermal Impedance
- 8.0 Thermal Conductivity
- High Breakdown Voltage
-
RTM-X22 | Pluggable Phase Change Pad
- 0.7 Thermal Impedance
- >50 Pluggable performance
- 0.15 - 0.22mm Thickness
-
Honeywell TA 3000
- Moisture cure
- Good thermal performance
- Adjusts to irregular surfaces