TG1500I | Thermal Grease

Main features

  • 0.03 Thermal Impedance
  • 1.5 Thermal Conductivity
  • 30μm BLT

Product Description

TG1500I Thermal Silicone Grease offers a thermal conductivity of 1.5 W/mK and a controlled bond line thickness of 30 micron @35psi, 50oC.  Its viscosity and excellent thixotropy make it fit for large–scale production with dispensing, screen printing and stencil printing. It is an excellent, option for thermally demanding applications that can support a >30um BLT.

TG1500I is used for applications with high power density requirements. It provides superior thermal performance with ease of use across a multitude of applications.  It is a stable homogeneous mixture under room temperature with an operating temperature range of -40oC to 150oC. Please note that this thermal grease contains solvent and requires a drying step.

Product Key Features:

  • Low thermal resistance (0.021°C-in²/W at 50 psi) — effectively address overheating and reliability issues
  • Maintains high reliability and performance across demanding environments and applications
  • Suitable for use in pneumatic dispensing and screen printing systems, supporting automated and high-volume manufacturing

Applications

  • Heat dissipation from heat-generating components (like CPUs and GPUs) to cooling solutions (like heat sinks).
Product Family

SOLSTICE TG1500I

1. Select Package Type

Loading pricing…

Product availability
EU Shipping in 8 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color Color
White
Specific Gravity Specific Gravity
2.7
Thermal Properties
Thermal Conductivity Thermal Conductivity
1.5 W/m.K
Thermal Impedance Thermal Impedance
0.03 °C·cm²/W
UL 94 Rating UL 94 Rating
V-0
Electrical Properties
Volume Resistivity Volume Resistivity
10000000000000 Ohms⋅cm
Physical Properties
Viscosity Viscosity
250000 mPa.s