Dow XIAMETER PMX 200

Harmonization Code : 2710199990 |

Dow XIAMETER PMX 200

Main features

  • 1,000 cSt Polydimethylsiloxane Fluid
  • Surface Tension of 21.2 dynes/cm
  • Dielectric Strength of 400 volts/mil

Product Description

XIAMETER™ PMX-200 Silicone Fluid 1000 cSt is a colorless, clear polydimethylsiloxane fluid with a nominal kinematic viscosity of 1,000 cSt. The silicone fluid combines low surface tension with water repellency, heat stability, dielectric performance, and resistance to shear breakdown. Its viscosity-temperature characteristics and chemical stability support use as a lubricant and mechanical fluid, while its spreading and release properties make it suitable for mold release, surface treatment, polish formulations, and foam-control applications.

Key features

  • Stable 1,000 cSt silicone fluid: Provides a nominal kinematic viscosity of 1,000 cSt with resistance to shear breakdown and a viscosity-temperature coefficient of 0.61.
  • Low surface tension and water repellency: A typical surface tension of 21.2 dynes/cm at 25°C supports spreading, wetting, release, and water-repellent performance.
  • Electrical and thermal properties: Provides a typical dielectric strength of 400 volts/mil at 25°C and an open-cup flash point above 326°C.

Applications / Suitable for

  • Elastomer and plastics lubrication
  • Mechanical and damping fluids
  • Electrical insulating fluids
  • Mold release and surface-active applications
  • Automotive, furniture, metal, and specialty polish formulations
  • Foam prevention and foam breaking

Technical Specifications

General Properties
Surface Tension Surface Tension
21.2 mN/m
Electrical Properties
Dielectric Strength Dielectric Strength
400 kV/mm
Volume Resistivity Volume Resistivity
1.0x10¹⁵ Ohms⋅cm

Additional Information

Technical properties

As-supplied properties

Typical properties of the 1,000 cSt grade in its supplied fluid state. Values are not intended for use as specification limits.

Property Value Unit Method / condition
Appearance Crystal clear — Typical
Kinematic viscosity 1,000 cSt Nominal grade
Specific gravity 0.970 — At 25°C (77°F)
Refractive index 1.4035 — At 25°C (77°F)
Flash point, open cup >326 (>620) °C (°F) Open cup
Pour point -50 (-58) °C (°F) Typical
Surface tension 21.2 dynes/cm At 25°C (77°F)
Volatile content 0.11 % At 150°C (302°F)
Viscosity-temperature coefficient 0.61 — Typical
Dielectric strength 400 volts/mil At 25°C (77°F)
Volume resistivity 1.0 × 1015 ohm-cm At 25°C (77°F)

Leading Brands Trust in Our Products and Services