STYCAST 2741

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

STYCAST 2741

Main features

  • Catalyst-Adjusted Cured Flexibility
  • Shock- and Impact-Resistant Potting
  • Room-Temperature or Accelerated Cure

Product Description

LOCTITE STYCAST 2741 Epoxy Encapsulant is a black, filled two-component system used with CAT 15 for electronic embedment, sealing, and cementing of glass, metals, plastics, and ceramics. Catalyst level controls the cured response, providing rigid, semi-rigid, and flexible options with typical work lives of 120 to 160 minutes at 25 deg C. Room-temperature and accelerated cure schedules support varied production timing. The cured configurations combine adjustable hardness with shock and impact resistance, electrical insulation, and service ranges matched to the selected formulation.

Key features

  • Catalyst-adjusted flexibility: CAT 15 loading selects rigid, semi-rigid, or flexible cured behavior.
  • Room-temperature cure option: The system cures in 16 to 24 hours at 25 deg C or faster with heat.
  • Multi-substrate assembly use: Supported substrates include glass, metals, plastics, and ceramics.

Applications

Applications include electronic embedment and the sealing or cementing of metals, ceramics, and plastics where adjustable flexibility and shock or impact resistance are required.

Product Family

STYCAST 2741

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for STYCAST 2741 with CAT 15; rigid, semi-rigid, and flexible formulations use different catalyst levels.

Property Value Unit Method / condition
Resin density 1.65 g/cm^3 Typical
Resin viscosity 225,000 mPa s (cP) Brookfield; typical
CAT 15 density 0.97 g/cm^3 Typical
CAT 15 viscosity 25,000 mPa s (cP) Brookfield; typical
Mixed viscosity 37,000 / 37,000 / 36,000 mPa s (cP) Rigid / semi-rigid / flexible formulations
Work life 120 / 140 / 160 minutes 100 g at 25 deg C; rigid / semi-rigid / flexible
Cure schedule 16 to 24 h at 25 deg C; 4 to 6 h at 45 deg C; 2 to 4 h at 65 deg C Typical alternatives
Technical properties

After-processing / final-state properties

Typical cured properties vary with the rigid, semi-rigid, or flexible formulation.

Property Value Unit Method / condition
Hardness 80 Shore D / 60 Shore D / 60 Shore A Rigid / semi-rigid / flexible formulations
Thermal conductivity 0.35 W/(m K) All three formulations
Operating temperature range -40 to 90 / -55 to 80 / -55 to 65 deg C Rigid / semi-rigid / flexible formulations
Water absorption 0.2 / 0.5 % 24-hour immersion; rigid / semi-rigid
Linear shrinkage 0.001 cm/cm Rigid, semi-rigid, and flexible formulations