STYCAST 2651-40FR

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

STYCAST 2651-40FR

Main features

  • Low-Viscosity Potting Process
  • Flame-Retardant Cured Encapsulation
  • Low-Temperature Operating Range

Product Description

LOCTITE STYCAST 2651-40FR Flame-Retardant Epoxy Encapsulant is a black, two-component epoxy system used with CAT 24LV for general electrical and electronic potting. The 100:16 by-weight mix has a typical mixed viscosity of 1,200 mPa s and a 60-minute work life at 25 deg C, providing a controlled window before room-temperature or accelerated cure. After cure, the material combines a -65 to 105 deg C operating range with Shore D 88 hardness, dielectric properties, and the grade's flame-retardant formulation. Processing and final values remain specific to the CAT 24LV configuration.

Key features

  • Low-viscosity mixed system: The CAT 24LV mixture has a typical viscosity of 1,200 mPa s.
  • Flame-retardant formulation: The 2651-40FR grade is the flame-retardant version of STYCAST 2651-40.
  • Low-temperature service range: The CAT 24LV system has an operating range of -65 to 105 deg C.

Applications

Applications include electrical and electronic potting where a flame-retardant epoxy system and the CAT 24LV processing profile are required.

Product Family

STYCAST 2651-40FR

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied and mixed values for STYCAST 2651-40FR with CAT 24LV.

Property Value Unit Method / condition
Resin viscosity 30,000 mPa s (cP) Brookfield; typical
Resin density 1.55 g/cm^3 Typical
Resin shelf life 6 months 25 deg C; from date of manufacture
Mix ratio by weight 100:16 STYCAST 2651-40FR:CAT 24LV
Mixed viscosity 1,200 mPa s (cP) Brookfield; typical
Mixed density 1.44 g/cm^3 Typical
Work life 60 minutes 100 g at 25 deg C
Cure schedule 8 to 16 h at 25 deg C; 2 h at 65 deg C Typical alternatives
Technical properties

After-processing / final-state properties

Typical cured properties for the CAT 24LV configuration.

Property Value Unit Method / condition
Operating temperature range -65 to 105 deg C CAT 24LV cured system
Hardness 88 Shore D Typical cured value
Glass transition temperature 58 deg C TMA
Coefficient of thermal expansion 64 10^-6/deg C TMA
Thermal conductivity 0.55 W/(m K) ASTM D2214
Water absorption 0.92 % Water boil
Volume resistivity >1 x 10^14 ohm cm 25 deg C
Dielectric constant / dissipation factor 4.27 / 0.03 1 MHz

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers