STYCAST 2651

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

STYCAST 2651

Main features

  • Catalyst-Selectable Cure Profiles
  • 45-Minute CAT 9 Work Life
  • NASA Outgassing Performance

Product Description

LOCTITE STYCAST 2651 Epoxy Encapsulant is a black, filled general-purpose dielectric epoxy resin for potting and encapsulation with a choice of compatible catalysts. With CAT 9, the system mixes 100:7 by weight, reaches a typical mixed viscosity of 32,000 cP, and provides a 45-minute working time at 25 deg C. The cured material combines electrical insulation, 0.66 W/(m K) thermal conductivity, 88 Shore D hardness, and service from -40 to 130 deg C. Documented NASA outgassing values support evaluation for demanding electronic and aerospace assemblies.

Key features

  • Catalyst-selectable processing: Compatible catalyst options support different mix, work-life, and cure requirements.
  • Dielectric thermal performance: The CAT 9 cured system combines insulation with 0.66 W/(m K) thermal conductivity.
  • Documented outgassing data: Typical TML and CVCM values support aerospace material evaluation.

Applications

Applications include general electrical and electronic potting, including assemblies requiring dielectric performance, thermal conduction, and documented outgassing data.

Product Family

STYCAST 2651

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

The table uses the CAT 9 formulation; other approved catalysts have different ratios, viscosities, work lives, and cure schedules.

Property Value Unit Method / condition
Product form Black filled dielectric epoxy resin Values below use CAT 9 catalyst
Resin viscosity 225,000 cP 25 deg C; Brookfield, spindle 7, 5 rpm
Resin specific gravity 1.65 Typical as supplied
Mix ratio 100:7 parts by weight Resin:CAT 9
Mix ratio 100:11.5 parts by volume Resin:CAT 9
Mixed viscosity 32,000 cP CAT 9; typical
Mixed specific gravity 1.56 CAT 9; typical
Working time 45 minutes CAT 9 at 25 deg C
Technical properties

After-processing / final-state properties

Typical cured properties for the CAT 9 formulation.

Property Value Unit Method / condition
Operating temperature -40 to 130 deg C CAT 9 cured formulation
Hardness 88 Shore D CAT 9 cured formulation
Water absorption 0.25 % 24-hour boil; CAT 9 cured formulation
Coefficient of thermal expansion 43.3 ppm/deg C TMA; CAT 9 cured formulation
Thermal conductivity 0.66 W/(m K) ASTM D2214; CAT 9 cured formulation
Volume resistivity 5 x 10^15 ohm cm 25 deg C; CAT 9 cured formulation
Dielectric strength 17.7 kV/mm CAT 9 cured formulation
Outgassing TML 0.37; CVCM 0.03 % Sample cured 8 hours at 25 deg C