STYCAST 1266

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

STYCAST 1266

Main features

  • Low-Viscosity Fine-Gap Impregnation
  • Optically Clear Encapsulation
  • Flexible Ambient or Heat Cure

Product Description

LOCTITE STYCAST 1266 Epoxy Encapsulant is a clear, two-component low-viscosity epoxy system for impregnation and encapsulation where optical clarity and flow into small tolerances are important. Parts A and B mix 100:28 by weight or 100:33 by volume to produce a typical mixed viscosity of 650 cP and a 30-minute working time at 25 deg C. The material can cure at ambient temperature or in one to two hours at 65 deg C, with an optional post-cure. After cure, it provides documented mechanical strength, moisture resistance, and electrical insulation.

Key features

  • Fine-gap impregnation: A typical mixed viscosity of 650 cP supports flow into narrow spaces.
  • Optically clear encapsulation: The clear system supports applications requiring visible components.
  • Flexible cure options: Ambient and heat-cure schedules support different production needs.

Applications

Applications include impregnation and encapsulation of electrical or electronic components, including assemblies with small tolerances and a need for optical clarity.

Technical Specifications

General Properties
Component System Component System
Two Part (Resin | Hardener)
Electrical Properties
Dielectric Strength Dielectric Strength
15.7 kV/mm
Volume Resistivity Volume Resistivity
1×10¹⁵ Ohms⋅cm
Other Properties
Storage Temperature Storage Temperature
25 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Property Value Unit Method / condition
Product form Two-component clear epoxy system Part A is clear amber; Part B is clear yellow
Mix ratio 100:28 parts by weight Part A:Part B
Mix ratio 100:33 parts by volume Part A:Part B
Part A viscosity 8,500 cP ASTM D2393
Part B viscosity 35 cP Typical
Mixed viscosity 650 cP 25 deg C; typical
Mixed specific gravity 1.12 Typical
Working time 30 minutes 100 g mass at 25 deg C
Technical properties

After-processing / final-state properties

Property Value Unit Method / condition
Hardness 75 Shore D ASTM D2240
Dielectric strength 15.7 kV/mm ASTM D149
Dielectric constant 3.0 60 Hz; ASTM D150
Dissipation factor 0.02 60 Hz; ASTM D150
Volume resistivity 1 x 10^15 ohm cm 25 deg C; ASTM D257
Flexural strength 138 N/mm^2 Typical cured value
Compressive strength 69 N/mm^2 Typical cured value
Tensile strength 41 N/mm^2 Typical cured value