SILASTIC 3112

Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated

SILASTIC 3112

Main features

  • 28,000 cP Base Viscosity
  • Adjustable Catalyst-Controlled Cure
  • Simple-Pattern Mold Making

Product Description

SILASTIC RTV-3112 Mold-Making Base is a white, general-purpose condensation-cure silicone base for producing simple molds without deep undercuts. The base has a typical viscosity of 280 poise (28,000 cP) and a specific gravity of 1.30 at 25 deg C, supporting pourable processing and reproduction of detailed patterns. A compatible catalyst is selected and added separately to establish the working and cure profile; the base is not a complete mold-making system by itself. Use is limited to mold geometries, catalyst ratios, release practices, and cure conditions validated for the intended pattern and casting material.

Key features

  • 28,000 cP base viscosity: Supports pourable mold preparation at 25 deg C
  • Separate catalyst control: Catalyst selection and ratio establish the working and cure profile
  • Detailed pattern reproduction: Low mixed viscosity supports replication of intricate features

Applications

General-purpose silicone mold making for simple patterns without deep undercuts, using a compatible catalyst and validated release and cure process.

Product Family

SILASTIC 3112

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color Color
White
Specific Gravity Specific Gravity
1.30
Physical Properties
Viscosity Viscosity
280 mPa.s
Mechanical Properties
Elongation Elongation
127 %

Additional Information

Technical properties

As-supplied / before-processing properties

The page entity is the mold-making base only; catalyst selection and cure conditions remain system-dependent.

Property Value Unit Method / condition
Color White As supplied
Viscosity 280 (28,000) poise (cP) At 25 deg C
Specific gravity 1.30 At 25 deg C
Reference mix ratio 10:1 base:catalyst by weight RTV-3010-S Catalyst reference formulation; catalyst sold separately

Leading Brands Trust in Our Products and Services