SILASTIC 164

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

SILASTIC 164

Main features

  • 1:1 mix ratio
  • UL 94 V-0 flame resistance
  • Electrical insulation performance

Product Description

SYLGARD™ 164 Silicone Elastomer is a two-part, 1:1 mix ratio, gray silicone encapsulant designed for potting and protecting electrical and electronic assemblies. The material combines good flowability, moderate thermal conductivity, flame resistance, and rapid room-temperature or heat-accelerated cure to support efficient manufacturing processes. Once cured, it forms a flexible silicone elastomer suitable for protecting components in power supplies, connectors, sensors, industrial controls, transformers, amplifiers, high-voltage resistor packs, and relay assemblies. Its UL 94 V-0 flammability rating, electrical insulation properties, and broad operating temperature capability make it suitable for demanding electronic encapsulation applications.

Key features

  • 1:1 mix ratio: Supports straightforward automated mixing, dispensing, and process control.
  • UL 94 V-0 flame resistance: Can be considered for applications requiring enhanced flame-retardant performance.
  • Electrical insulation performance: Provides dielectric strength of 19 kV/mm and volume resistivity of 1.1 × 10¹³ ohm·cm.

Applications / Suitable for

  • Power supplies
  • Connectors
  • Sensors
  • Industrial controls
  • Transformers
  • Amplifiers
  • High-voltage resistor packs and relays

Technical Specifications

Electrical Properties
Dielectric Strength Dielectric Strength
19 kV/mm
Volume Resistivity Volume Resistivity
1.1 E + 13 Ohms⋅cm
Thermal Properties
Thermal Conductivity Thermal Conductivity
0.64 W/m.K
UL 94 Rating UL 94 Rating
V0

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured two-part silicone system before processing and cure.

Property Value Unit Method / Condition
Mix Ratio 1:1 Parts Part A : Part B
Viscosity (Part A) 8,925 cP Base component
Viscosity (Part B) 9,175 cP Catalyst component
Working Time 14 minutes 25°C snap time
Cure Time 0.6 hours 25°C
Shelf Life 15 months Stored at 25°C
Technical properties

After-processing / final-state properties

Typical cured silicone elastomer properties.

Property Value Unit Method / Condition
Durometer Hardness 61 Shore A Cured elastomer
Dielectric Strength 19 kV/mm Electrical insulation property
Volume Resistivity 1.1E+13 ohm·cm Typical value
Thermal Conductivity 0.64 W/m·K Typical value
Linear CTE 225 ppm/°C By TMA
Flammability Rating UL 94 V-0 N/A UL classification