SIKABIRESIN CF234

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

SIKABIRESIN CF234

Main features

  • 24-part hardener weight ratio
  • 0.43 g/cm3 Part B density
  • Honeycomb edge-fill system hardener

Product Description

SikaBiresin CF234 Part B Hardener is the green amine paste component for the two-part CF230/CF234 epoxy edge-filling system. It is mixed with CF230 Part A at 24 parts hardener to 100 parts resin by weight. Part B has a typical specific gravity of 0.43 at 25 deg C; the combined material has a typical 11-minute pot life at the same temperature. The system forms a lightweight, smooth paste for honeycomb edge filling, cell densification around inserts, and localized sandwich-panel repairs. Final mechanical, thermal, flame-test, shrinkage, and machinability data apply only after CF234 is combined and cured with the specified CF230 Part A resin.

Key features

  • Controlled hardener ratio: Use 24 parts CF234 to 100 parts CF230 by weight
  • Low-density Part B: The green amine paste has a typical specific gravity of 0.43 at 25 deg C
  • Short mixed pot life: The 116 g CF230/CF234 mixture has an 11-minute pot life at 25 deg C

Applications

Edge filling of aluminum and other honeycomb sandwich structures; core-cell densification for insert anchoring; localized sandwich-panel repairs.

Technical Specifications

General Properties
Appearance Appearance
paste
Chemistry Type Chemistry Type
amine
Color Color
green
Component System Component System
two
Specific Gravity Specific Gravity
0.43

Additional Information

Technical properties

As-supplied / before-processing properties

Part B properties are separated from processing values for the complete CF230/CF234 system.

Property Value Unit Method / condition
Composition Amine CF234 Part B
Aspect Paste As supplied
Color Green CF234 Part B
Specific gravity 0.43 g/cm3 At 25 deg C
System mix ratio by weight 100:24 CF230 Part A:CF234 Part B
Mixed-system pot life 11 minutes 116 g mixture at 25 deg C
Shelf life 12 months Original unopened container at 15-25 deg C