ROYAL M6325

Main features

  • One-part paste application
  • 15 to 45 minute tack-free
  • Resilient elastomeric bond

Product Description

Royal Silaprene M6325 Adhesive/Sealant is a one-part gray polychloroprene adhesive/sealant supplied in a paste extrusion grade for room-temperature application. The material develops a tack-free surface in 15 to 45 minutes under ambient conditions and reaches an initial set in about four hours. It can be applied with a caulking gun or suitable pressure-pumping equipment and does not require component mixing, priming, or heating. After solvent evaporation, the elastomeric material forms a resilient bond and seal that continues to build strength over time.

Key features

  • One-part paste: Applies without component mixing, priming, or heating
  • Fast surface set: Tack-free in 15 to 45 minutes under ambient conditions
  • Resilient elastomer: Forms a flexible bond and seal after solvent evaporation
Product Family

ROYAL M6325

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type Chemistry Type
Polychloroprene
Solids Solids
50 %
Specific Gravity Specific Gravity
1.1
Thermal Properties
Operating Temperature Operating Temperature
-51 to 121 °C