PP-52008G-060-TSF Nylon Peel Ply

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

PP-52008G-060-TSF Nylon Peel Ply

Main features

  • 100% Nylon 6,6 Peel Ply
  • Fine Surface Impression
  • FIN 060 Scoured Heat-Set Fabric

Product Description

PP-52008G-060-TSF Nylon Peel Ply is a 100% nylon 6,6 fabric designed for vacuum-bag composite layups and metal-to-metal bonding structures. The peel ply melts at approximately 480°F (249°C) and leaves a fine surface impression after removal to support subsequent priming and secondary bonding operations. The FIN 060 construction has a scoured and heat-set finish and is available in precision-slit widths of 56 inches or less.

Key features

  • Nylon 6,6 construction: Manufactured from 100% nylon 6,6 fiber with an approximate melting point of 480°F (249°C).
  • Bond-preparation surface: Leaves a fine surface impression suitable for subsequent priming and secondary bonding.
  • Scoured and heat-set finish: FIN 060 is supplied with the manufacturer-designated NAT scoured and heat-set finish.
  • Precision-slit availability: Available in precision-slit widths of 56 inches or less.

Applications / Suitable for

  • Vacuum-bag composite layups
  • Metal-to-metal bonding structures
  • Surface preparation before priming and secondary bonding
Product Family

PP-52008G-060-TSF

Loading pricing…

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Published product properties. The source states that the information is not to be construed as a specification.

Property Value Unit Method / condition
Material 100% nylon 6,6 fiber — Code 52008
Finish FIN 060 – NAT, scoured and heat-set — Manufacturer finish designation
Fiber melting point Approximately 480 (249) °F (°C) Nylon 6,6 fiber
Roll width 58 (147.3) minimum in (cm) ASTM D3774
Roll length 300 (274.3) maximum yd (m) Published roll format
Weight 1.7 (57.6) minimum oz/yd² (g/m²) ASTM D3776
Finished count – warp 101 (39.8) minimum ends/in (ends/cm) ASTM D3775
Finished count – fill 82 (32.3) minimum picks/in (picks/cm) ASTM D3775
Tensile strength – warp 115 (511.8) minimum lb/in (N) ASTM D5034, grab method
Tensile strength – fill 105 (467.3) minimum lb/in (N) ASTM D5034, grab method
Thickness 0.004–0.005 (0.102–0.127) in (mm) ASTM D1777
pH 4.5–7.0 — AATCC 81
Extractable materials 0.5 maximum % ASTM D2257, petroleum ether