PLEXUS MA440

Harmonization Code : 3904.61.00.00 | Polytetrafluoroethylene plates / sheets / film / tape / strip, self-adhesive, in rolls

PLEXUS MA440

Main features

  • Self-Leveling Two-Part System
  • 15 MPa Typical Tensile Strength
  • 121 deg C Air Service Limit

Product Description

Plexus MA440 Methacrylate Adhesive uses a two-part, self-leveling methacrylate system for structural bonding of thermoplastic, metal, and composite assemblies. The uncured material has a reported density of 0.980 g/cm3. Typical cured values include 15.0 MPa tensile strength, 20% elongation, a 0.300 GPa elastic modulus, and 9.50 MPa cohesive lap-shear strength under the stated ASTM methods. A maximum air service temperature of 121 deg C is also reported. These characteristics position MA440 for structural joints where a flowable adhesive and a balance of strength and moderate elongation are needed.

Key features

  • Self-leveling application: The two-part adhesive flows to wet structural joint surfaces.
  • Cured mechanical balance: Typical cured properties include 15.0 MPa tensile strength and 20% elongation.
  • Elevated-temperature range: The reported maximum air service temperature is 121 deg C.

Applications / Suitable for

  • Structural bonding of thermoplastic, metal, and composite assemblies.
Product Family

PLEXUS MA440

Loading pricing…

Technical Specifications

General Properties
Density (g) Density (g)
0.980 g/cm3
Mechanical Properties
Elongation Elongation
20 %

Additional Information

Technical properties

As supplied / before processing

Rows distinguish the uncured MA440 material and its two-part application form.

Property Value Unit Method / condition
Component countTwo-part-Part A adhesive and Part B activator
Application formSelf-leveling-Uncured adhesive
Density0.980g/cm3Uncured material
Technical properties

After processing / final state

Values describe the cured material under the stated ASTM method or service condition.

Property Value Unit Method / condition
Tensile strength15.0MPaASTM D638
Elongation at break20%ASTM D638
Elastic modulus0.300GPaASTM D638
Cohesive lap-shear strength9.50MPaASTM D1002
Maximum air service temperature121deg CCured material