PLEXUS H4110

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

PLEXUS H4110

Main features

  • Extended 8-12 Minute Work Window
  • Non-Sag Gel Placement
  • Elastic Mixed-Material Bonding

Product Description

Plexus H4110 is a two-part, 1:1 hybrid adhesive supplied as a non-sagging gel for elastic semi-structural bonding. It provides an 8-12 minute work time at 25 deg C for positioning composites, thermoplastics, metals, wood, concrete, and cement. The low-odor, low-exotherm formulation supports controlled application where a more elastic bond is preferred over a rigid structural joint. Its gel consistency limits slump during placement and keeps the mixed adhesive within the intended bond area across supported mixed-material assemblies.

Key features

  • 8-12 Minute Work Window: Allows measured part positioning at 25 deg C.
  • Non-Sag Gel Control: Maintains controlled placement during assembly.
  • Elastic Semi-Structural Bond: Forms an elastic bond for supported mixed-material assemblies.

Applications

Applications include bonding composites, thermoplastics, metals, wood, concrete, and cement.

Technical Specifications

Physical Properties
VOC VOC
0 %
Mechanical Properties
Elongation Elongation
150 %
General Properties
Component System Component System
Two part
Other Properties
Storage Temperature Storage Temperature
10 - 24 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Property Value Unit Method / condition
System formTwo-part non-sagging gelAs supplied and mixed for application
Mix ratio by volume1:1Adhesive to activator
Work time8-12minutesAt 25 deg C
Exotherm characteristicLowMixed adhesive
Odor characteristicLowMixed adhesive