PERMABOND UV683

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

PERMABOND UV683

Main features

  • Controlled Doming and Encapsulation
  • Rapid Tack-Free UV Cure
  • High-Transmittance Cured Coating

Product Description

Permabond UV683 is a colorless UV-curable acrylate coating and doming compound for smart-card microchips and electronic-component encapsulation. Its 1,000 to 1,600 mPa s viscosity at 25 deg C supports doming application, while cure across 320 to 420 nm produces a tack-free surface. Typical tack-free time ranges from 1 to 15 seconds under the listed lamp conditions. The cured coating provides more than 98% light transmittance, 12 to 14 N/mm^2 tensile strength, more than 50% elongation, and 50 to 65 Shore D hardness for optically clear protective applications.

Key features

  • Doming-Grade Viscosity: Viscosity is 1,000 to 1,600 mPa s at 25 deg C.
  • Rapid Tack-Free Cure: Typical tack-free time is 1 to 15 seconds under the listed lamp conditions.
  • High-Transmittance Coating: The cured coating provides more than 98% light transmittance.

Applications

Applications include coating and doming, smart-card microchip coating, and encapsulation of electronic components.

Technical Specifications

General Properties
Appearance Appearance
Colorless
Refractive index Refractive index
>1.490
Specific Gravity Specific Gravity
1.1
Physical Properties
Viscosity Viscosity
1,000-1,600 mPa.s
Mechanical Properties
Elongation Elongation
>50 %
Chemical Properties
Water Absorption Water Absorption
<2 %
Other Properties
Storage Temperature Storage Temperature
2 - 7 °C
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
55 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Fixture time depends on lamp output, distance, and substrate transmission.

Property Value Unit Method / condition
Chemical compositionAcrylateAs supplied
AppearanceColorlessAs supplied
Viscosity1,000 to 1,600mPa sAt 25 deg C
Specific gravity1.1As supplied
Typical fixture time1 to 7secondsListed UV lamp conditions
Typical tack-free time1 to 15secondsListed UV lamp conditions
Cure wavelength320 to 420nmMatch lamp output to the photoinitiator
Technical properties

After-processing / final-state properties

Values are typical cured properties for the stated methods and substrates.

Property Value Unit Method / condition
Tensile strength12 to 14N/mm^2ISO 37
Light transmittance>98%Cured coating
Refractive index>1.490Cured coating
Elongation at break>50%ISO 37
Hardness50 to 65Shore DISO 868
Water absorption<2%ISO 62; 2 hours in boiling water
Glass transition temperature55deg CDSC; 20 deg C/min rate