PERMABOND QFS16

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PERMABOND QFS16

Main features

  • 5-Second Steel Set Time
  • Faster Cure Through Gaps
  • Reduced Plastic Stress Cracking

Product Description

Permabond QFS16 is a colorless cyanoacrylate activator for shortening set time on closely mated parts, porous surfaces, gaps, and wire-tacking assemblies. It is applied to one component by wiping, spraying, or dipping and allowed to evaporate before adhesive is placed on the untreated surface. With a 100 cP ethyl-2-cyanoacrylate at 23 deg C, typical set time is 5 seconds on gap-free steel and 40-60 seconds across a 5 mil gap. The formulation also reduces stress cracking, surface discoloration, and adhesive frosting on supported plastic parts.

Key features

  • Rapid Steel Set: Provides a typical 5-second set on gap-free steel under stated conditions.
  • Gap and Porous-Surface Cure: Accelerates cyanoacrylate cure through gaps and on porous materials.
  • Reduced Plastic Surface Effects: Helps limit stress cracking, discoloration, and frosting on supported plastics.

Applications

Applications include porous or poorly mated parts, gap bonding, wire tacking, excess-fillet cure, and supported plastic assemblies.

Technical Specifications

General Properties
Color Color
Colorless
Specific Gravity Specific Gravity
0.68
Thermal Properties
Flash Point Flash Point
-2 °C
Other Properties
Storage Temperature Storage Temperature
5 - 25 °C

Additional Information

Technical properties

As supplied / before processing

Property Value Unit Method / condition
Product typeCyanoacrylate activatorAs supplied
ColorColorlessAs supplied
Specific gravity0.68As supplied
Flash point-2deg CAs supplied
Application methodWipe, spray, or dip one componentAllow full evaporation before bonding
Storage temperature5 to 25deg CRecommended storage range
Technical properties

After processing / final state

Set-time values apply to 100 cP ethyl-2-cyanoacrylate at 23 deg C; the control row is identified separately.

Property Value Unit Method / condition
Set time - steel, no gap5secondsAt 23 deg C with 100 cP ethyl-2-cyanoacrylate and QFS16
Set time - steel, 5 mil gap40-60secondsAt 23 deg C with 100 cP ethyl-2-cyanoacrylate and QFS16
Set time - steel, no gap, control10-15secondsAt 23 deg C without QFS16
Set time - Buna-N, no gap10secondsAt 23 deg C with 100 cP ethyl-2-cyanoacrylate and QFS16
Set time - phenolic, no gap5secondsAt 23 deg C with 100 cP ethyl-2-cyanoacrylate and QFS16

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers