PERMABOND HL126

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PERMABOND HL126

Main features

  • Water-Thin Wicking Threadlocker
  • Warm-Weld/Casting Porosity Sealing
  • MIL-S-22473E/MIL-S-46163A/ASTM D5363 Compliance

Product Description

Permabond® HL126 is a water-thin, extremely low-viscosity anaerobic threadlocker designed specifically for wicking into pre-assembled parts via capillary action. By penetrating tight-fitting metallic threads after assembly, it effectively locks fasteners in place to prevent vibration-induced loosening. Furthermore, its penetrating characteristics make it an ideal sealant for weld porosities, as the uncured material easily flows into micro-pores to form a durable, 100% solid environmental seal upon curing.

Key features

  • Wicking grade viscosity: The ultra-low viscosity (10-30 cP) allows application post-assembly and enables deep penetration into micro-porosities and tight tolerances.
  • Military and ASTM approved: Formulated to meet the stringent lot requirements of MIL-S-22473E (Grade AA), MIL-S-46163A (Type III Grade R), and ASTM D5363.
  • Weld sealing capability: Excellent for sealing weld porosity; it wicks into the warm voids and cures rapidly without solvents to establish a new, pressure-resistant seal.

Applications / Suitable for

  • Post-assembly locking of set screws, bolts, and fasteners
  • Sealing weld porosity and casting micro-pores
  • Acting as a tamper-proof agent for assembled joints
Product Family

PERMABOND HL126

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance Appearance
Green
Chemistry Type Chemistry Type
Methacrylate esters
Specific Gravity Specific Gravity
1.0
Physical Properties
Viscosity Viscosity
10 -30 mPa.s
Other Properties
Maximum gap fill Maximum gap fill
0.05 mm
Maximum thread size Maximum thread size
M10 ½
Electrical Properties
Dielectric Strength Dielectric Strength
11 kV/mm
Thermal Properties
Thermal Conductivity Thermal Conductivity
0.19 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Methacrylate esters - -
Appearance Green - Liquid
Viscosity 10-30 mPa.s (cP) at 25°C
Specific Gravity 1.0 - -
Maximum Gap Fill 0.05 mm (0.001 in)
Maximum Thread Size M10 - (3/8")
Flash Point > 100 °C (212°F)
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Handling Strength Time 15 minutes M10 steel at 23°C
Full Strength Time 24 hours M10 steel at 23°C
Breakaway Torque Strength 14 N-m M10 steel (ISO 10964) (125 in.lb)
Prevailing Torque Strength 34 N-m M10 steel (ISO 10964) (300 in.lb)
Shear Strength 10-20 MPa Steel collar & pin (ISO 10123) (1450-2900 psi)
Coefficient of Thermal Expansion 90E-6 mm/m/°C -
Dielectric Strength 11 kV/mm -
Thermal Conductivity 0.19 W/(m.K) -

Leading Brands Trust in Our Products and Services