PERMABOND 940

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PERMABOND 940

Main features

  • Non-Frosting Alkoxyethyl Formulation
  • Low-Odor Cyanoacrylate Bonding
  • Fast Multi-Substrate Fixturing

Product Description

Permabond® 940 Cyanoacrylate is a low-odor, non-frosting, alkoxyethyl-based cyanoacrylate adhesive engineered to improve worker comfort and maintain a clean aesthetic. This 100% reactive, single-component adhesive cures rapidly at room temperature, eliminating the unsightly white fogging (blooming) that commonly occurs with standard cyanoacrylates on hot and humid days. It is surface-insensitive and rapidly bonds a wide range of materials, including plastics, metals, elastomers, and acidic surfaces.

Key features

  • Low odor formulation: Alkoxyethyl chemistry significantly reduces irritating fumes, improving worker comfort during application.
  • Non-frosting/Non-fogging: Eliminates the white residue (blooming) adjacent to the bondline, ensuring a flawless aesthetic appearance on finished parts.
  • Fast room-temperature cure: Provides rapid fixture times (e.g., 2-5 seconds on Neoprene/NBR and 10-15 seconds on steel), eliminating the need for mixing or heat.

Applications / Suitable for

  • Applications requiring a clean, fog-free aesthetic finish
  • Environments where low-odor adhesives are necessary for worker comfort
  • Rapid bonding of plastics, metals, and elastomers
Product Family

PERMABOND 940

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance Appearance
Liquid
Chemistry Type Chemistry Type
Alkoxyethyl cyanoacrylate
Color Color
Colourless
Specific Gravity Specific Gravity
1.1
Physical Properties
Viscosity Viscosity
3-10 mPa.s mPa.s
Mechanical Properties
Impact Strength Impact Strength
3-5 kJ/m² mm
Thermal Properties
Linear thermal expansion Linear thermal expansion
90 x 10^-6 mm/mm/°C
Thermal Conductivity Thermal Conductivity
0.1 W/m.K
Electrical Properties
Dielectric Strength Dielectric Strength
25 kV/mm
Maximum gap fill Maximum gap fill
0.05 mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Alkoxyethyl cyanoacrylate - -
Appearance Colorless - Liquid
Viscosity 3-10 cP at 25°C (mPa.s)
Specific Gravity 1.1 - -
Maximum Gap Fill 0.05 mm (0.002 in)
Flash Point 80-93 °C (176°F - 199.94°F)
Volatile Organic Compound < 2 % 20 g/L (Estimated)
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Fixture/Handling Time 10-15 seconds Steel, Aluminium, PVC, Phenolic resin, ABS
Full Strength 24 hours -
Shear Strength 16-20 N/mm² Steel (ISO 4587) (2300-2900 psi)
Impact Strength 3-5 kJ/m² ASTM D-950 (1.4-2.4 ft-lb/in²)
Hardness 85 Shore D ISO 868
Dielectric Constant 3 - DIN 53483 at 1MHz
Dielectric Strength 25 kV/mm DIN 53481
Coefficient of Thermal Expansion 90E-6 mm/mm/°C -
Coefficient of Thermal Conductivity 0.1 W/(m.K) -

Leading Brands Trust in Our Products and Services