PERMABOND 790

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PERMABOND 790

Main features

  • 2 to 3-Second Handling Time
  • Surface-Insensitive Acidic-Substrate Bonding
  • Low-Viscosity Wicking Post-Assembly Bonding

Product Description

Permabond® 790 Cyanoacrylate is an extremely fast-setting, low-viscosity, surface-insensitive adhesive designed to rapidly bond a wide variety of substrates. Its specialized formulation readily bonds acidic surfaces such as wood and plated metals, along with plastics, ceramics, and elastomers. Featuring a highly penetrative wicking viscosity, this 100% reactive, solvent-free adhesive is ideal for post-assembly applications and minimizes the occurrence of frosting and fogging during cure.

Key features

  • Extremely fast setting: Single-component formula polymerizes rapidly upon contact with surface moisture, delivering fixture handling times of 2-3 seconds on steel and rubber.
  • Surface insensitive: Expertly engineered to rapidly bond notoriously difficult acidic surfaces, including wood and plated materials.
  • Low wicking viscosity: The exceptionally low 2 cP viscosity enables superior wicking action, making it perfectly suited for post-assembly penetration and application.

Applications / Suitable for

  • Bonding acidic surfaces such as wood and plated materials
  • Adhering plastics, metals, ceramics, and elastomers
  • Post-assembly applications utilizing wicking penetration

Technical Specifications

General Properties
Appearance Appearance
Liquid
Chemistry Type Chemistry Type
Ethyl cyanoacrylate
Color Color
Colourless
Specific Gravity Specific Gravity
1.1
Physical Properties
Viscosity Viscosity
2 mPa.s mPa.s
Mechanical Properties
Impact Strength Impact Strength
3-5 kJ/m² mm
Thermal Properties
Thermal Conductivity Thermal Conductivity
0.1 W/m.K
Electrical Properties
Dielectric Strength Dielectric Strength
25 kV/mm
Maximum gap fill Maximum gap fill
0.05 mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Ethyl cyanoacrylate - -
Appearance Colorless - -
Viscosity 2 cP at 25°C (mPa.s)
Specific Gravity 1.1 - -
Maximum Gap Fill 0.05 mm (0.002 in)
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Fixture/Handling Time 2-3 seconds Steel, Buna N Rubber, Phenolic
Full Strength 24 hours -
Shear Strength 18-22 N/mm² Steel (ISO 4587) (2600-3200 psi)
Impact Strength 3-5 kJ/m² ASTM D-950 (1.4-2.4 ft-lb/in²)
Hardness 85 Shore D ISO 868
Dielectric Constant 2.5 - at 10kHz
Dielectric Strength 25 kV/mm -