PERMABOND 2K

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

PERMABOND 2K

Main features

  • 1 mPa s Low Viscosity
  • Eight-Hour Mixed Working Life
  • Visible Red Coverage

Product Description

PERMABOND 2K Primer is a two-component, red liquid surface treatment for preparing metal, glass, plastic, and composite substrates before bonding with engineering adhesives. The mixed primer has a typical viscosity of 1 mPa s and specific gravity of 1.0, allowing a thin, visible coating that indicates surface coverage. Its mixed working life is 8 hours, and unopened material has a 24-month shelf life when stored at 5-25 deg C. It is used before compatible epoxy, acrylic, polyurethane, and other engineering adhesive systems; the primer itself does not form the bonded joint.

Key features

  • Visible red coverage: The red liquid provides a visual indication of primer wetting and surface coverage.
  • Low-viscosity application: A typical viscosity of 1 mPa s supports thin surface treatment.
  • Eight-hour mixed life: The combined primer remains usable for up to 8 hours.

Applications / Suitable for

  • Preparing metal and glass surfaces before adhesive bonding
  • Preparing plastic and composite surfaces
  • Use before compatible epoxy, acrylic, and polyurethane adhesive systems

Technical Specifications

Other Properties
Storage Temperature Storage Temperature
5 - 25 °C
General Properties
Color Color
Red
Component System Component System
Two
Specific Gravity Specific Gravity
1.0
Physical Properties
Viscosity Viscosity
1 mPa.s
Thermal Properties
Flash Point Flash Point
55 °C

Additional Information

Technical properties

As-supplied and working properties

Property Value Unit Method / condition
Appearance Red liquid Mixed primer
Viscosity 1 mPa s Typical
Specific gravity 1.0 Typical
Flash point 55 deg C Typical
Mixed working life 8 h After combining components
Shelf life 24 months Unopened; stored at 5-25 deg C