PERMABOND 101

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

PERMABOND 101

Main features

  • 2 to 3 mPa s Viscosity Range
  • 2 to 10-Second Fixturing Time
  • 25 kV/mm Dielectric Strength

Product Description

PERMABOND® 101 Cyanoacrylate Adhesive is an ultra-low-viscosity, single-component ethyl cyanoacrylate adhesive for wicking into close-fitting joints and bonding pre-assembled parts. It cures rapidly when confined as a thin film between surfaces, with typical handling strength reached in 2–10 seconds depending on the substrate. The adhesive is suitable for plastics, rubber, and metals and has a maximum recommended gap fill of 0.05 mm. After cure, it provides high shear strength on steel and other substrates, 85 Shore D hardness, and electrical insulation properties suitable for industrial assembly applications.

Key features

  • Ultra-low viscosity: A 2–3 mPa·s viscosity supports capillary wicking into closely fitted and pre-assembled joints.
  • Fast fixture time: Typical handling strength is achieved in 2–10 seconds, depending on the bonded substrate.
  • Multi-material bonding: Supports bonding of plastics, rubber, and metals, with documented shear data on steel, aluminum, zinc, ABS, PVC, polycarbonate, and phenolic.

Applications / Suitable for

  • Pre-assembled components
  • Close-fitting plastic parts
  • Wicking and penetrating applications
  • High-speed industrial assembly
  • Bonding plastics, rubber, and metals
Product Family

PERMABOND 101

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance Appearance
Liquid
Chemistry Type Chemistry Type
Ethyl cyanoacrylate
Color Color
Colourless
Specific Gravity Specific Gravity
1.1
Physical Properties
Viscosity Viscosity
2-3 mPa.s
Mechanical Properties
Impact Strength Impact Strength
3-5 kJ/m² mm
Thermal Properties
Thermal Conductivity Thermal Conductivity
0.1 W/m.K
Electrical Properties
Dielectric Strength Dielectric Strength
25 kV/mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured and curing properties. Values are guideline information and are not product specifications.

Property Value Unit Method / condition
Chemical composition Ethyl cyanoacrylate — Single-component adhesive
Appearance Colorless liquid — As supplied
Viscosity 2–3 mPa·s At 25 °C; equivalent to cP
Specific gravity 1.1 — Typical uncured value
Maximum gap fill 0.05 mm Equivalent source value 0.002 in
Fixture time — steel 3–5 s Time to 0.3 N/mm² shear strength
Fixture time — Buna N rubber 2–5 s Time to 0.3 N/mm² shear strength
Full strength 24 h Typical full-strength development
Technical properties

As-supplied / before-processing properties

Typical uncured and curing properties. Values are guideline information and are not product specifications.

Property Value Unit Method / condition
Chemical composition Ethyl cyanoacrylate — Single-component adhesive
Appearance Colorless liquid — As supplied
Viscosity 2–3 mPa·s At 25 °C; equivalent to cP
Specific gravity 1.1 — Typical uncured value
Maximum gap fill 0.05 mm Equivalent source value 0.002 in
Fixture time — steel 3–5 s Time to 0.3 N/mm² shear strength
Fixture time — Buna N rubber 2–5 s Time to 0.3 N/mm² shear strength
Full strength 24 h Typical full-strength development