OPTOLINQ LE-EP246D | Optically Transparent Epoxy Resin

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

OPTOLINQ LE-EP246D | Optically Transparent Epoxy Resin

Main features

  • Low working time and viscosity
  • Perfect surface gloss
  • Good chemical resistance

Product Description

OPTOLINQ LE-EP246D is a two-component, low viscosity epoxy with excellent handling properties, chemical resistance, and high-gloss finish. It is ideal for potting, casting, sealing, encapsulation, and adhesive applications in electronic components, as well as for general industrial uses requiring extended work life.

The hardener of LE-EP246D does not form insoluble, white solids even after being exposed to air. The cured surface remains oil-free while maintaining excellent gloss retention. Additionally, OPTOLINQ LE-EP246D offers excellent electrical insulation properties under high humidity conditions, withstands exposure to a wide range of chemicals and solvents, and complies to RoHS 2011/65/EU Directive.

Applications

  • Potting, casting, and encapsulation of electronic components
  • General industrial sealing and coating applications
  • Adhesive for transparent, chemical-resistant assemblies
  • Applications requiring extended work life, chemical resistance, and optical clarity

 

Product Family

OPTOLINQ LE-EP246D

1. Select Package Type

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance Appearance
Liquid, colorless
Mix Ratio Mix Ratio
100:33
Pot Life Pot Life
8 hours
Refractive index Refractive index
1.532
Thermal Properties
Degradation temperature Degradation temperature
324 °C
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
90 °C
Weight Loss @ 300°C Weight Loss @ 300°C
2.7 %
Electrical Properties
Surface Resistivity Surface Resistivity
5e14 Ohms/sq
Volume Resistivity Volume Resistivity
4.5e15 Ohms⋅cm
Mechanical Properties
Elongation Elongation
10 %
Chemical Properties
Water Absorption Water Absorption
1.59 %
Physical Properties
Viscosity Viscosity
262.5 mPa.s

Additional Information

LE-EP246D Additional Technical Specifications

Property Value Unit

Spectral Transmission

at 1,200-4,000 nm

at 900-1,200 nm

at 550-900 nm

80

80

>96

%

Toughness

5

J/m2

Notched Izod Impact Strength

5.9

J/m

LE-EP246D Recommended Curing Conditions

Property Value Unit
Mixing Ratio (A:B) 100:33 by weight
Pot Life (25℃) 8 hour(s)
Through Cure Time (25℃) 5-7 day(s)
Through Cure Time (80℃) 3 hour(s)

Leading Brands Trust in Our Products and Services