MOLYKOTE GN

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE GN

Main features

  • Mineral-Oil Solid-Lubricant Assembly Paste
  • 0.08 Press-Fit Friction Coefficient
  • 2,800 N Four-Ball Weld Load

Product Description

MOLYKOTE® G-N Plus Paste is a black mineral-oil solid-lubricant paste for assembly, press fitting, running-in, and low-motion lubrication of metal components. The supplier reports an ISO 2137 unworked penetration of 280–310 mm/10, a 2,800 N four-ball weld load, an Almen-Wieland OK load above 20,000 N, and a press-fit coefficient of friction of 0.08 with no chatter. Solid-lubricant temperature guidance extends from -25°C to 450°C and up to 630°C with reduced air access; these limits do not imply unchanged carrier or paste properties throughout the range. Apply a thin layer to clean contact surfaces, rub it into the metal to improve adhesion, and do not mix it with greases or oils.

Key features

  • High-load bench performance: DIN 51350 four-ball weld load of 2,800 N and Almen-Wieland OK load above 20,000 N.
  • Controlled friction: Press-fit coefficient of friction of 0.08 with no chatter; screw-test values of 0.12 at the thread and 0.06 under the head.
  • Solid-lubricant temperature guidance: -25°C to 450°C, or up to 630°C with reduced air access, based on the temperature resistance of the solid lubricants.
  • Wear and water-resistance data: 0.75 mm wear scar under an 800 N four-ball load and DIN 51807 static water-resistance rating of 2-90.
  • High surface coverage: Supplier-stated covering capacity of 40 m²/kg when applied as a controlled thin film.
  • Fluorinated-material statement: Formulated with no intentional PTFE or other PFAS.

Applications / Suitable for

  • Press-fit assembly and fitting of machine elements, bearings, washers, wheels, flanges, and bolts
  • Running-in lubrication for new machines and gearboxes
  • Threaded spindles, splined shafts, toothed gears, worm gears, transmission gears, and screws
  • Valves, pumps, machine-tool guides, and components with rare or slight movement
  • Drilling, sawing, and thread-cutting operations

Technical Specifications

No specifications available.

Additional Information

High-load assembly and running-in paste

MOLYKOTE® G-N Plus Paste

A black mineral-oil paste containing solid lubricants and a thickener for assembly, press fitting, running-in, and low-motion lubrication of metallic components. Its product-specific load and friction data support evaluation where high contact pressure, controlled assembly friction, stick-slip avoidance, fretting protection, and later dismantling are important.

Mineral-oil paste NLGI 1–2 2,800 N weld load 0.08 press-fit friction 40 m²/kg coverage No intentional PTFE or PFAS
Approved product image showing MOLYKOTE G-N Plus Paste packaging and label.

MOLYKOTE® G-N Plus Paste is a black solid-lubricant paste for assembly and running-in of metal components.

As-supplied paste properties

Lubricant system
Mineral oil / solid lubricants
A paste carrier and concentrated solid-lubricant system for metal assembly, running-in, and low-motion contacts.
Consistency
NLGI 1–2
Current supplier classification; ISO 2137 unworked penetration is 280–310 mm/10.
Surface coverage
40 m²/kg
Supplier-stated covering capacity for controlled thin-film application.
Property Value Unit Method / condition
Product form Solid-lubricant paste — Mineral-oil carrier with solid lubricants and thickener
Color Black — Typical commercial appearance
NLGI grade 1–2 — Current supplier product classification
Unworked penetration 280–310 mm/10 ISO 2137
Density 1.35 g/ml ISO 2811 at 20°C
Surface-covering capacity 40 m²/kg Supplier-stated characteristic
Intentional PTFE / PFAS None — Supplier formulation statement

Typical values and supplier classifications are not specification limits. Confirm the required delivery form, surface finish, and application quantity for the intended assembly process.

Load, friction, and temperature performance

Four-ball weld load
2,800 N
DIN 51350 part 4 bench result; it is not an equipment load rating.
Almen-Wieland OK load
>20,000 N
Condition-specific result from the Almen-Wieland machine.
Press-fit friction
µ 0.08
Press-fit test result reported with no chatter under the stated test configuration.
Property Value Unit Method / condition
Solid-lubricant temperature guidance -25 to +450 °C Temperature resistance of the solid lubricants
Reduced-air temperature guidance Up to +630 °C Temperature resistance of the solid lubricants with reduced air access
Four-ball weld load 2,800 N DIN 51350 part 4
Four-ball wear scar 0.75 mm DIN 51350 part 5; 800 N load
Almen-Wieland OK load >20,000 N Almen-Wieland machine
Almen-Wieland frictional force 2,600 N Almen-Wieland machine
Press-fit coefficient of friction 0.08; no chatter µ Press-fit test
Screw-test coefficient — thread 0.12 µ Erichsen test; M12, class 8.8, blackened surface
Screw-test coefficient — head 0.06 µ Erichsen test; M12, class 8.8, blackened surface
Static water resistance 2-90 rating DIN 51807 part 1

The temperature figures describe the resistance of the solid lubricants and do not establish unchanged carrier-oil, consistency, friction, wear, or service-life performance across the full range. Bench results remain specific to their methods and conditions.

Application process

Apply a controlled film to clean metal surfaces

Prepare the contact area before applying the paste. The supplier recommends a thin, worked-in film rather than the larger quantities associated with conventional grease lubrication.

Clean: Remove contamination from the sliding surfaces or contact areas before application.
Apply: Use a brush, cloth, synthetic sponge, or chamois to distribute a thin layer across the intended metal contact.
Work into the surface: Vigorous rubbing into the metal improves adhesion of the paste film.
Control quantity and mixing: Do not apply in excess as with grease lubrication, and do not mix with greases or oils.
Technician rubbing a thin black solid-lubricant paste into a cleaned metal press-fit, threaded, or sliding contact surface.

Use a thin, uniform film and work the paste into the cleaned metal surface rather than applying it as a bulk grease fill.

Storage and Handling

Store between 0°C and 40°C in the original unopened container. Usable life is 60 months from the date of production. Review the current safety data and container label before handling; use local exhaust ventilation and appropriate protective gloves and eye/face protection. The current SDS states that heating above 150°C in air can form formaldehyde vapors, so applicable ventilation and exposure controls are required.

Applications

Assembly, running-in, and low-motion applications

The documented application scope covers metallic contacts where assembly friction, high contact pressure, intermittent movement, running-in behavior, fretting risk, or later dismantling are important. Final suitability depends on the material pair, geometry, surface condition, load, temperature, atmosphere, and applied film quantity.

Metal press-fit and bolted assembly with a thin black paste applied to mating surfaces, threads, bearing seats, and flange contacts.
Press-fit and bolted assemblies
For press-fit production and fitting of roller bearings, washers, wheels, flanges, bolts, and related machine elements. Product-specific press-fit and screw-test coefficients provide controlled test data for assembly evaluation.
Gearbox internals showing threaded spindles, splined shafts, toothed gears, worm gears, and transmission components prepared for running-in.
Machine and gearbox running-in
Used as a running-in lubricant for new machines and gearboxes, including threaded spindles, splined shafts, toothed gears, worm gears, transmission gears, and screws.
Valve, pump, machine-tool guide, and metalworking setup representing intermittent-motion lubrication and drilling, sawing, or thread cutting.
Low-motion components and metalworking
Documented uses include valves, pumps, machine-tool guides, components moved only rarely or slightly, and drilling, sawing, or thread-cutting operations.
Next steps

Evaluate MOLYKOTE® G-N Plus Paste for your metal assembly

Krayden can help review the material pair, surface finish, press-fit or threaded geometry, target friction behavior, contact pressure, movement profile, temperature and atmosphere, corrosion exposure, film quantity, application method, and existing lubricant before a trial on assembly, running-in, gearbox, guide, valve, pump, or metalworking components.

Leading Brands Trust in Our Products and Services