MOLYKOTE G-5042

Main features

  • Effective Purple Silicone Grease
  • Siloxane Base Oil and Lithium Soap Thickener
  • Long-Term Silicone-Grease Lubrication

Product Description

MOLYKOTE® G-5042 Silicone Automotive Service Grease is a purple silicone grease formulated with a siloxane base oil and a lithium soap thickener. Designed specifically for the long-term lubrication of metal-to-plastic and plastic-to-plastic material pairings, it delivers excellent low-temperature properties and significantly reduces friction in automotive assemblies. Its distinct color makes it easy to visually confirm that the grease has been successfully applied to control cables, starter motor overrun clutches, and windshield wiper motor gears.

Key features

  • Broad temperature range: Provides reliable, long-term lubrication across an operating temperature range of -50°C to +170°C (-58°F to +338°F).
  • Low friction and plastic compatibility: Delivers a low coefficient of friction (0.02 vs. PA66, 0.03 vs. POM) and is highly compatible with numerous plastics and elastomers used in modern automotive design.
  • Visual detection: The purple color of the grease acts as a built-in visual indicator to ensure proper application on assembly lines.

Applications / Suitable for

  • Long-term lubrication of metal/plastic and plastic/plastic pairings
  • Automotive starter motor overrun clutches and control cables
  • Automotive windshield wiper motor gears
  • Use within centralized lubrication systems

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Siloxane base oil, lithium soap thickener - Silicone grease
Appearance / Color Purple - Grease
Worked Penetration 300-350 mm/10 Worked 60 (ISO 2137)
Base Oil Kinematic Viscosity 100 mm²/s at 25°C (DIN 51 562)
Specific Gravity / Relative Density 0.97 g/ml at 20°C (ISO 2811)
Flash Point 100 °C (212°F) Closed cup
Shelf Life 60 months From the date of production when stored unopened between 0°C and 40°C
Technical properties

After-processing / in-service properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Service Temperature Range -50 to +170 °C (-58 to +338 °F)
Dropping Point >= 200 °C IP 396/02
Flow Pressure 225 mbar at -50°C (Kesternich method, DIN 51805)
Coefficient of Friction (vs. POM) 0.03 µ Steel ball vs. POM (Ball-plate test, Ø 12.7 mm, 5 N, 10 mm/s, 1 h) (CTM 1089)
Coefficient of Friction (vs. PA66) 0.02 µ Steel ball vs. PA66 (Ball-plate test, Ø 12.7 mm, 5 N, 10 mm/s, 1 h) (CTM 1089)
Corrosion Resistance <= 1 - Degree of corrosion, SKF-Emcor method (DIN 51 802)
Bleed 4.0 % 24 h at 150°C (ASTM D6184)
Evaporation 1.8 % 24 h at 150°C (ASTM D6184)