MOLYKOTE G-4700

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE G-4700

Main features

  • Extreme-Load Bearing Lubrication
  • PAO Synthetic Base Oil and Lithium Complex Thickener
  • Industrial Plastic/Elastomer Compatibility

Product Description

MOLYKOTE® G-4700 Extreme Pressure Synthetic Grease is a high-performance, light-consistency synthetic grease formulated with a polyalphaolefin (PAO) base oil, a lithium complex thickener, and fortified with molybdenum disulfide (MoS₂) solid lubricants. Engineered to handle extreme loads, vibration, and shock loading, it offers a higher load-carrying capacity, greater wear resistance, and longer service life than conventional petroleum-based lubricants.

Key features

  • Extreme-pressure performance: Designed specifically to withstand extreme loads and shock loading, boasting a high four-ball weld load of 3,700 N.
  • Wide operating range & compatibility: Delivers reliable lubrication across a broad temperature range of -40°C to 177°C (-40°F to 350°F) and provides good compatibility with most industrial plastics and elastomers.
  • Industry approvals: Meets Cincinnati Machine P-64 and NLGI GC-LB specifications. Formulated without intentional polytetrafluoroethylene (PTFE) or per- and polyfluoroalkyl substances (PFAS).

Applications / Suitable for

  • Rolling element and plain bearings
  • Pivot pins, cams, guides, and ways
  • Drive screws, gears, splines, and other heavily loaded machine elements

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition PAO base oil, lithium complex thickener, MoS2 - Organic grease
Appearance / Color Black / Dark grey - Grease
NLGI Consistency Class 2 - DIN 51 818
Worked Penetration 265-295 mm/10 at 25°C (77°F), W/60 (ASTM D217)
Base Oil Viscosity (40°C) 150 cSt ASTM D445
Base Oil Viscosity (100°C) 20 cSt ASTM D445
Specific Gravity / Relative Density 0.87 g/ml at 25°C (77°F) (ISO 2811)
Flash Point > 230 °C (446°F) Closed cup
Usable Life 60 months Stored at or below 35°C (95°F) in original unopened containers
Technical properties

After-processing / in-service properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Service Temperature Range -40 to 177 °C (-40 to 350°F) Approximate
Dropping Point > 285 °C (> 545°F) (ASTM D2265)
Low-Temperature Torque .024 Nm at -40°C (-40°F) (ASTM D4693)
Four-Ball Wear 0.64 mm 40 kg, 1,200 rpm (ASTM D2266)
Four-Ball EP Weld Load 3,700 N Minimum (ASTM D2596)
Dn Value 350,000 mm/min Estimated (bearing ID x rpm)
Oil Bleed 3.9 wt% 24 hours at 100°C (212°F) (FD 791-32/2)
Oil Evaporation 0.44 wt% 24 hours at 100°C (212°F) (FD 791-32/2)

Leading Brands Trust in Our Products and Services