MOLYKOTE G-3407

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE G-3407

Main features

  • -40 to 200 deg C Service Range
  • Brake-Caliper Guide-Pin Lubrication
  • 120-Hour No-Rust Test Result

Product Description

MOLYKOTE® G-3407 Caliper Pin Grease is a light-green synthetic grease formulated with polyalkylene glycol (PAG) base oil and a lithium-complex thickener for automotive brake-caliper guide pins and other supported metal-to-metal contacts. Its documented service-temperature range is -40°C to 200°C. Product-specific test data include less than 5% bleed and evaporation after 24 hours at 150°C, less than 5% water washout at 80°C, no rust after 120 hours in ASTM B117 testing, and bounded EPDM volume- and hardness-change limits after 72 hours at 150°C. Apply to clean contact surfaces using a clean brush or manual or automated dispensing equipment, and confirm compatibility with the exact elastomer and assembly conditions before use.

Key features

  • Caliper guide-pin lubrication: PAG-based grease intended for automotive brake-caliper mounting pins and supported metal-to-metal pairings.
  • Wide service-temperature range: Documented for operation from -40°C to 200°C.
  • High-temperature retention data: Less than 5% bleed and less than 5% evaporation after 24 hours at 150°C.
  • EPDM compatibility evidence: Maximum 8% volume change and maximum 8 Shore A hardness change after 72 hours at 150°C under the stated test.
  • Water and corrosion test results: Less than 5% water washout at 80°C and no rust after 120 hours in ASTM B117 testing.

Applications / Suitable for

  • Automotive brake-caliper guide and mounting pins
  • Supported metal-to-metal sliding contacts in brake-caliper assemblies
  • Manual or automated grease-dispensing processes for caliper-pin lubrication

Technical Specifications

No specifications available.

Additional Information

Automotive brake lubricant

MOLYKOTE® G-3407 Caliper Pin Grease

A PAG-based, lithium-complex synthetic grease for automotive brake-caliper guide pins and supported metal-to-metal contacts. The product combines a -40°C to 200°C service range with high-temperature retention, water-washout, corrosion, low-temperature torque, and EPDM compatibility data for application-specific evaluation.

PAG synthetic base oil Lithium-complex thickener -40°C to 200°C Light-green grease No intentional PTFE or PFAS
Approved product image showing the exact MOLYKOTE G-3407 Caliper Pin Grease package and label.

MOLYKOTE® G-3407 Caliper Pin Grease is supplied as a light-green synthetic grease for caliper guide-pin lubrication.

As-supplied grease properties

Lubricant system
PAG / lithium complex
Synthetic polyalkylene-glycol base oil with a lithium-complex thickener.
Consistency
260–310 mm/10
Unworked and worked penetration ranges under CTM 0191 / ASTM D217.
Appearance
Light green
Typical as-supplied color; the current U.S. SDS describes the product as green.
Property Value Unit Method / condition
Color Light green — As supplied
Penetration, unworked 260–310 mm/10 CTM 0191 / ASTM D217
Penetration, worked 260–310 mm/10 CTM 0191 / ASTM D217
Specific gravity 1.00 ± 0.1 g/mL CTM 0044 at 25°C
Dropping point >250 °C ASTM D566; test result, not a service-temperature limit

Typical values are not specification limits.

Service performance and compatibility

Service temperature
-40°C to 200°C
Supplier-documented operating range; performance should be evaluated under the actual brake-caliper duty cycle.
EPDM compatibility
≤8% / ≤8 Shore A
Maximum volume and hardness changes after 72 hours at 150°C under CTM 0130 / ASTM D4289.
Water and corrosion
<5% / no rust
Water washout at 80°C and ASTM B117 corrosion result after 120 hours.
Property Result Unit Method / condition
Bleed <5 % ASTM D6184; 24 h at 150°C
Evaporation <5 % CTM 0033A; 24 h at 150°C
Corrosion protection No rust — ASTM B117; 120 h
Low-temperature torque, starting 2,000 max. gf·cm ASTM D1478 at -20°C
Low-temperature torque, running 800 max. gf·cm ASTM D1478 at -20°C
Water washout <5 % ASTM D1264 at 80°C
EPDM volume change 8 max. % CTM 0130 / ASTM D4289; 72 h at 150°C
EPDM hardness change 8 max. Shore A CTM 0130 / ASTM D4289; 72 h at 150°C

Results are specific to the listed methods and conditions. EPDM compatibility should not be generalized to every elastomer grade, formulation, aged component, or mixed-lubricant condition.

Application guidance

Prepare and dispense for caliper guide-pin lubrication

Apply the grease to clean contact surfaces using conventional grease-application methods. Control the amount and distribution according to the caliper design, component geometry, elastomer system, and validated assembly process.

Surface preparation: Remove contamination and old lubricant residues that could interfere with the validated grease and elastomer combination; ensure the contact area is clean before application.
Application methods: Use a clean brush or manual or automated dispensing equipment.
Compatibility control: Confirm the exact EPDM or other elastomer grade, existing lubricant, temperature exposure, and assembly conditions before production use.
Technician applying a controlled amount of grease to a clean automotive brake-caliper guide pin before assembly.

The final visual should show clean guide-pin preparation and controlled grease placement without implying a universal fill quantity.

Storage and handling

Store at or below 40°C in the original unopened container. Usable life is 60 months from the date of production under the stated storage condition. Review the current safety data and container label before handling, use adequate ventilation, and keep the product away from strong oxidizing agents.

Next steps

Evaluate MOLYKOTE® G-3407 for your brake-caliper guide-pin system

Krayden can help review caliper geometry, operating temperature, elastomer grade, existing lubricant, water exposure, dispensing method, and validation requirements. Contact us to discuss product fit, samples, technical data interpretation, or an application-specific evaluation plan.