MOLYKOTE G-3000

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE G-3000

Main features

  • Dual-Mass-Flywheel High-Shear Grease
  • -40 to 180 deg C Service Range
  • 2,200 N Four-Ball Weld Load

Product Description

MOLYKOTE® G-3000 Synthetic Grease is a beige, approximately NLGI 3 grease based on synthetic oil and a lithium-complex thickener for dual-mass flywheels. The product is characterized by high shear and centrifugal stability, an approximately 400 mm²/s base-oil viscosity at 40°C, and a documented service range of -40°C to 180°C with short-term exposure to 220°C. Condition-specific data include a 2,200 N four-ball weld load, a 0.7 mm wear scar under 400 N, SKF-Emcor corrosion rating 0/0, approximately 0% oil bleeding, and 0.6% evaporation after 24 hours at 150°C. The 300°C dropping point is a test result and is not the maximum continuous service temperature.

Key features

  • Dual-mass flywheel grease: Synthetic-oil/lithium-complex formulation developed specifically for DMFW lubrication.
  • Mechanical stability: ISO 2137 penetration changes from 223 mm/10 unworked to 253 mm/10 after 100,000 strokes.
  • Temperature capability: Documented -40°C to 180°C service range with short-term exposure to 220°C.
  • Load, wear, and corrosion data: 2,200 N weld load, 0.7 mm wear scar under 400 N, and SKF-Emcor rating 0/0.
  • High-temperature retention data: Approximately 0% oil bleeding and 0.6% evaporation after 24 hours at 150°C.

Applications / Suitable for

  • Dual-mass flywheels (DMFWs)

Technical Specifications

No specifications available.

Additional Information

Synthetic grease for dual-mass flywheels

MOLYKOTE® G-3000 Synthetic Grease

A beige, approximately NLGI 3 grease based on synthetic oil and a lithium-complex thickener, developed for dual-mass flywheels. High shear and centrifugal stability, a documented -40°C to 180°C service range, and condition-specific retention, wear, and corrosion data support evaluation for rotational and torsional DMFW duty.

Approx. NLGI 3 Synthetic oil / lithium complex ~400 mm²/s at 40°C -40°C to 180°C Short-term 220°C
Approved product image showing the exact MOLYKOTE G-3000 Synthetic Grease package and label.

MOLYKOTE® G-3000 Synthetic Grease is formulated for dual-mass flywheel lubrication.

As supplied

Grease composition and consistency

Grease system
Approx. NLGI 3
Synthetic base oil thickened with lithium-complex soap and oxidation inhibitors.
Base-oil viscosity
~400 mm²/s
Typical value at 40°C; this is base-oil viscosity, not finished-grease consistency.
Mechanical stability
30 mm/10 change
Difference between 223 unworked and 253 worked penetration after 100,000 strokes.
Property Value Unit Method / condition
Color Beige — As supplied
NLGI consistency class Approx. 3 — DIN 51818
Unworked penetration range 215–230 mm/10 ISO 2137
Unworked penetration 223 mm/10 ISO 2137
Worked penetration 253 mm/10 ISO 2137; after 100,000 strokes
Difference from unworked penetration 30 mm/10 ISO 2137
Density at 20°C 1.0 g/mL ISO 2811
Base-oil viscosity at 40°C ~400 mm²/s DIN 51562
Usable life 60 months At 23°C in original unopened containers

Typical values are not specification limits. NLGI class, penetration, and base-oil viscosity describe different properties and should not be treated as interchangeable.

In service

Temperature, retention, load, wear, and corrosion data

Service temperature
-40°C to 180°C
Supplier-documented service range; short-term exposure is listed separately at 220°C.
High-temperature retention
~0% bleed / 0.6% evaporation
Typical results after 24 hours at 150°C under FDS 791-32/2.
Load and corrosion results
2,200 N / 0/0
Four-ball weld load and SKF-Emcor corrosion rating under the stated methods.
Property Value Unit Method / condition
Service temperature range -40 to +180 °C Supplier-documented service range
Short-term temperature 220 °C Short-term exposure; not continuous service
Dropping point 300 °C ASTM D566; test transition, not service limit
Flow pressure at -20°C 675 mbar DIN 51805, Kesternich method
Four-ball weld load 2,200 N DIN 51350 T.4
Wear scar under 400 N load 0.7 mm DIN 51350 T.5
Degree of corrosion 0/0 — DIN 51802, SKF-Emcor method
Oil bleeding Approx. 0 % FDS 791-32/2; 24 h at 150°C
Oil evaporation 0.6 % FDS 791-32/2; 24 h at 150°C

Results are condition-specific laboratory values. The dropping point is not a continuous operating limit, and bench load or wear results do not establish equipment capacity or field service life.

Application context

Designed for dual-mass flywheel lubrication

Dual-mass flywheels combine sustained rotation with torsional oscillation. MOLYKOTE® G-3000 Synthetic Grease is documented specifically for this application and is described as having high shear and centrifugal stability, characteristics directly relevant to grease exposed to rotational and oscillatory duty.

Application validation should use the actual thermal profile, rotational speed, oscillation amplitude, contact materials, lubricant quantity, sealing design, and existing lubricant. The -40°C to 180°C service range is separate from the 220°C short-term limit and the 300°C dropping-point test result.

Representative cutaway of a dual-mass flywheel showing the primary mass, secondary mass, and internal spring-damping region.

Representative dual-mass flywheel architecture; actual geometry and lubricant placement vary by design.

Product resource

Vehicle powertrain lubrication selection guide

Smart Lubrication™ for Vehicle Powertrain Systems
This four-page DuPont guide maps lubrication design needs across bearings, dual-mass flywheels, pistons, actuators, joints, fasteners, and electrical interfaces. Its powertrain selection table identifies MOLYKOTE® G-3000 Grease for DMFW applications. It is useful for powertrain designers, application engineers, and lubricant-selection teams reviewing related MOLYKOTE® technologies.
Next steps

Evaluate MOLYKOTE® G-3000 Synthetic Grease for your DMFW design

Krayden can help review the operating-temperature profile, rotational and oscillatory duty, contact materials, grease quantity, sealing approach, and validation plan for a dual-mass flywheel application. Contact us to discuss technical data, sample requirements, or application-specific lubricant selection.