MOLYKOTE G-1067

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE G-1067

Main features

  • Low-Friction Plastic-Compatible PAO Grease
  • 50 to 120 deg C Service Range
  • Automotive Lubrication Applications

Product Description

MOLYKOTE® G-1067 Grease is a white, synthetic lubricating grease formulated with a polyalphaolefin (PAO) base oil, a lithium soap thickener, and white solid lubricants. Specifically designed for automotive body and plastic components, this smooth, buttery grease provides exceptional lubricity and noise-damping properties. It excels in applications involving plastic-to-metal and plastic-to-plastic interfaces, particularly glass-fiber-reinforced plastics (GFRP).

Key features

  • Excellent plastic compatibility: Highly compatible with most plastics, providing low friction and reduced noise at steel/GFRP interfaces.
  • Broad temperature range: Delivers reliable lubrication across a wide service temperature range of -50°C to 120°C (-45°F to 257°F).
  • Clean formulation: Formulated without intentional polytetrafluoroethylene (PTFE) or per- and polyfluoroalkyl substances (PFAS).

Applications / Suitable for

  • Automotive rail parts, including sunroof and moonroof slides
  • Lubrication of glass-fiber-reinforced plastic (GFRP) parts against steel or other plastics
  • Industrial assembly and appliance slides, guides, and linear drives

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Polyalphaolefin (PAO) oil, lithium soap thickener, white solid lubricants - Organic grease
Appearance / Color White / Off-white to beige - Smooth, buttery grease
NLGI Consistency Class 2 - -
Worked Penetration 302 - 342 mm/10 Worked 60 strokes (JIS K 2220 / ASTM D217)
Base Oil Viscosity 31.2 cSt at 40°C
Relative Density 0.83 - Water = 1
Flash Point > 100 °C (212°F) Seta closed cup
Shelf Life 36 months Stored closed below 40°C in original containers
Technical properties

After-processing / in-service properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Service Temperature Range -50 to 120 °C (-45 to 257°F)
Dropping Point 210 °C (410°F) (JIS K 2220 / ASTM D566)
Bleed 0.0  % 24 hrs at 100°C (JIS K 2220 / ASTM D566)
Evaporation 0.1 - 0.4 % 22 hrs at 99°C (JIS K 2220 / ASTM D566)
Copper Corrosion Test 1a - 24 hrs at 100°C (JIS K 2220)
Four Ball Wear Scar 0.67  mm 1,200 rpm, 392 N, 1 hr (75°C) (ASTM D2266)
Low-Temperature Torque (Starting) 46  mN*m at -40°C (JIS K 2220 / ASTM D1478)
Low-Temperature Torque (Running) 22  mN*m at -40°C (JIS K 2220 / ASTM D1478)