MOLYKOTE EM-50L

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE EM-50L

Main features

  • Broad Plastic Compatibility
  • 100% Silicone-Free PAO Grease
  • Low-Seepage Long-Service Lubrication

Product Description

MOLYKOTE® EM-50L Grease is an NLGI 1 lubricating grease specially developed for plastic components and precision equipment. Formulated with a polyalphaolefin (PAO) synthetic base oil and a lithium soap thickener, this translucent white grease is highly effective at acting as a damper grease to reduce noise in moving parts, such as plastic gears. Furthermore, its completely silicone-free composition ensures it will not cause contact point failures in sensitive electrical applications.

Key features

  • Plastic compatibility and noise reduction: Highly compatible with most plastics and specifically formulated to dampen and reduce noise generated by plastic gears.
  • Silicone-free formulation: Does not contain silicone, preventing the widespread issue of contact point failures in nearby electrical components.
  • Clean, long-life lubrication: Designed for long service life with low seepage, making it ideal for applications where cleanliness is strictly required.

Applications / Suitable for

  • Automobiles and electrical appliances containing plastic parts
  • Precision equipment, audio equipment, and office equipment
  • Use as a damper grease to reduce noise in moving components

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Polyalphaolefin base oil, lithium soap thickener - Silicone-free
Appearance / Color Translucent, white - Grease
NLGI Consistency Class 1 - -
Base Oil Viscosity 1,050 mm²/s at 40°C
Worked Penetration 325 - Worked 60 times (JIS K 2220)
Density 0.84 g/cm³ JIS K 2220 (Relative density 0.84)
Flash Point > 100 °C Seta closed cup (212 °F)
Shelf Life 36 months From date of production when stored unopened in a cool, dark place
Technical properties

After-processing / in-service properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Service Temperature Range -40 to 150 °C JIS K 2220
Drop Point 195 °C JIS K 2220
Bleed 2.5 % 100°C, 24 hours (JIS K 2220)
Evaporation 3.0 % 99°C, 22 hours (JIS K 2220)
Oxidation Resistance 0.02 MPa 99°C, 100 hours (JIS K 2220)
Copper Corrosion 1A - 100°C, 24 hours (JIS K 2220)
Four Ball Weld Load 1,400 N 1,500 rpm/1 minute (ASTM D2596)
Four Ball Wear Scar 0.71 mm 1,200 rpm, 392 N, 1 hour (ASTM D2266)
Low Temperature Torque (Starting) 290 mNm at -40°C (JIS K 2220)
Low Temperature Torque (Running) 140 mNm at -40°C (JIS K 2220)