MOLYKOTE E-PASTE

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE E-PASTE

Main features

  • 560 kg Four-Ball OK Load
  • ABS, Polycarbonate, Nylon, Polyacetal Compatibility
  • -50 to 150 deg C Service Range

Product Description

MOLYKOTE® E Paste is a light-yellow synthetic hydrocarbon lubricating paste with specially formulated solid lubricants for metal/metal, metal/plastic, and plastic/plastic contacts in electromechanical assemblies. It has a documented useful temperature range of -50°C to 150°C and is intended for sliding surfaces, threaded connections, gears, bearings, and oscillating mechanisms such as automotive sunroofs. Typical test data include a 560 kg four-ball OK load, a 0.50 mm wear scar under the stated four-ball conditions, more than 20,000 LFW-1 oscillating cycles, and a coefficient of friction of 0.08 after 6,000 cycles. Apply to solvent-cleaned surfaces by brush, burnishing, grease gun, or automated dispensing, and verify compatibility with the exact plastic grade and service conditions.

Key features

  • Wide documented temperature range: Useful from -50°C to 150°C, with static and kinetic torque data measured at -40°C.
  • Load and wear test data: Four-ball OK load of 560 kg and 0.50 mm wear scar at 1,740 rpm, 40 kg, and 1 hour.
  • Oscillating-contact performance: More than 20,000 cycles in the stated LFW-1 test and a coefficient of friction of 0.08 after 6,000 cycles.
  • Documented plastic test results: No cracking or color change for ABS, polycarbonate, nylon, and polyacetal after 500 hours at 60°C under bending stress.
  • Low measured retention losses: 1.0% bleed and 0.2% evaporation after 24 hours at 100°C.
  • Flexible application: Brush, burnishing, grease-gun, or automated dispensing methods.

Applications / Suitable for

  • Automotive sunroof guides and oscillating sliding mechanisms
  • Electromechanical sliding surfaces and guides
  • Metal/plastic and plastic/plastic gears and bearing contacts
  • Threaded connections requiring lubricated assembly
  • Precision mechanisms using ABS, polycarbonate, nylon, or polyacetal components, subject to application-specific validation

Technical Specifications

No specifications available.

Additional Information

Synthetic hydrocarbon lubricating paste

MOLYKOTE® E Paste

A light-yellow, heavy-duty paste with a synthetic hydrocarbon carrier and solid lubricants for metal/metal, metal/plastic, and plastic/plastic contacts. It is designed for electromechanical sliding, threaded, gear, bearing, and oscillating interfaces where load carrying, wear control, broad temperature capability, and verified compatibility with selected plastics are important evaluation factors.

Synthetic hydrocarbon paste NLGI 2 -50°C to 150°C 560 kg OK load Oscillating-contact data Selected-plastic test results
Approved product image showing MOLYKOTE E Paste packaging and label.

MOLYKOTE® E Paste is a light-yellow synthetic hydrocarbon paste for lubricating mixed-material electromechanical contacts.

As-supplied paste properties

Lubricant system
Synthetic hydrocarbon / solid lubricants
Paste for metal and selected plastic interfaces in electromechanical mechanisms.
Consistency
NLGI 2
Current supplier classification; the TDS reports worked penetration of 280 after 60 strokes.
Retention data
1.0% bleed / 0.2% evaporation
Typical results after 24 hours at 100°C under the stated test conditions.
Property Value Unit Method / condition
Product form Synthetic hydrocarbon paste — Specially formulated solid lubricants in a synthetic hydrocarbon carrier
Color Light yellowish — As supplied
Consistency classification NLGI 2 — Current supplier classification; worked penetration is 280
Worked penetration 280 0.1 mm 60 strokes
Specific gravity 1.18 g/cm³ Typical value
Bleed 1.0 % After 24 hours at 100°C
Evaporation 0.2 % After 24 hours at 100°C

Typical values are not specification limits. Bleed and evaporation are separate condition-specific measurements and should not be converted directly into service-life or contamination claims.

Load, wear, and oscillating performance

Four-ball OK load
560 kg
Typical value at 1,500 rpm for 1 minute; it is a bench-test endpoint, not an equipment load rating.
Oscillating endurance
>20,000 cycles
LFW-1 test at 90° angle, 600 lb, 75 cpm, and Rc60.
Low-temperature torque
2,500 / 600 gf·cm
Static and kinetic torque values measured at -40°C.
Property Value Unit Method / condition
Useful temperature range -50 to 150 °C Supplier-documented range; do not infer constant friction or life across the full range
Static torque 2,500 gf·cm Low-temperature torque at -40°C
Kinetic torque 600 gf·cm Low-temperature torque at -40°C
Four-ball wear scar 0.50 mm 1,740 rpm, 40 kg load, 1 hour
Four-ball OK load 560 kg 1,500 rpm, 1 minute
LFW-1 oscillating endurance >20,000 cycles 90° angle, 600 lb, 75 cpm, Rc60
Coefficient of friction 0.08 µ LFW-1 result after 6,000 cycles
Copper corrosion 1a rating After 24 hours at 100°C
Polystyrene foam test No change — After 24 hours at 60°C

These results describe the stated laboratory methods and conditions. Compare products only when test geometry, load, speed, temperature, duration, and endpoint are equivalent.

Material evaluation

Plastic compatibility evidence

The supplied TDS reports no cracking or color change for four plastic families in a bending-stress test after 500 hours at 60°C. The results support initial material screening but do not establish universal compatibility across all grades, additives, molded-in stress, aging states, temperatures, or lubricant combinations.

Tested material Reported result Test condition
ABS resin No crack; no color change Bending-stress test after 500 hours at 60°C
Polycarbonate No crack; no color change Bending-stress test after 500 hours at 60°C
Nylon No crack; no color change Bending-stress test after 500 hours at 60°C
Polyacetal No crack; no color change Bending-stress test after 500 hours at 60°C
Application check: Evaluate the exact plastic or elastomer grade, colorant and additive package, stress state, temperature, exposure duration, and any existing lubricant before production use.
Application process

Prepare a clean interface and apply by the required method

Application starts with solvent cleaning of the contact surface. Select brush, burnishing, grease-gun, or automated dispensing according to the mechanism and production process, then control distribution at the actual sliding, threaded, gear, or bearing interface.

Surface preparation: Clean the surface with an appropriate solvent and allow it to dry before applying the paste.
Application methods: Apply by brush, burnishing, grease gun, or automated dispensing.
Validation: Confirm application quantity, contact coverage, exact plastic grade, temperature, motion, load, and compatibility with any existing lubricant in the intended assembly.

 

Storage and handling

Review the current safety data and container label before handling. Use appropriate ventilation, avoid prolonged or repeated skin contact, and keep the product away from strong oxidizing agents. The supplied TDS directs users to the current Sales Specification for shelf-life information; confirm the applicable storage and shelf-life requirements before use.

Applications

Electromechanical lubrication applications

MOLYKOTE® E Paste is documented for metal/metal, metal/plastic, and plastic/plastic substrates in electromechanical mechanisms. Final selection should consider the exact material pair, motion, load, temperature, contact geometry, production method, and existing lubricant.

Automotive sunroof guide or track with plastic and metal sliding components.
Automotive sunroof guides and tracks
The paste is specifically documented for automotive sunroof mechanisms. Its oscillating-test evidence and metal/plastic compatibility data are relevant to repeated low-amplitude motion, while the exact guide material and application quantity still require assembly-level validation.
Plastic gear and bearing interface inside an electromechanical assembly.
Gears and bearing contacts
Suitable evaluation contexts include metal/plastic and plastic/plastic gears and bearings in electromechanical equipment. The 0.50 mm four-ball wear result and selected-plastic test data support screening, but do not replace gear- or bearing-specific load, speed, noise, and life testing.
Threaded connection and sliding guide in a compact precision mechanism.
Threaded connections and sliding surfaces
Brush, burnishing, grease-gun, or automated application can place the paste at threaded and sliding contacts. The 560 kg OK-load result and broad temperature range are decision inputs for heavily loaded contacts, not universal assembly-load or service-life guarantees.
Next steps

Evaluate MOLYKOTE® E Paste for your material pair and motion profile

Krayden can help review the exact plastic or metal grades, oscillating or sliding motion, temperature range, load and wear evidence, application method, and existing lubricant. Contact us to discuss sample needs, product comparison, dispensing considerations, or an assembly-specific evaluation plan.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers