MOLYKOTE D-96

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

MOLYKOTE D-96

Main features

  • Transparent Water-Based PTFE Dry Film
  • 100,000-Cycle No-Noise Pairing Result
  • -40 to 150 deg C Service Range

Product Description

MOLYKOTE® D-96 Anti-Friction Coating is a transparent, water-based, air-curing dry-film lubricant developed to control squeak and friction at low-load automotive interior interfaces. The PTFE-containing coating is intended for slow movements or vibration between combinations such as painted surfaces, plastics, metals, and leather. Apply it to clean, degreased surfaces by spray, dip-spinning, or brushing at a recommended dry-film thickness of 5–20 µm. At 23°C, the wet film is touch-dry after approximately 10 minutes and fully cured after 120 minutes; hot air at 60–80°C can reduce touch-dry time to about 2 minutes. The cured film has a documented service range of -40°C to 150°C. VDA 230-206 testing reported no noise for the listed material pairings under the stated test conditions, including a 100,000-cycle durability test for PVC foil against PC-ABS.

Key features

  • Water-based transparent coating: Supports friction and noise control while retaining a transparent finish.
  • Controlled thin-film application: Recommended dry-film thickness of 5–20 µm using spray, dip-spinning, or brush application.
  • Air-curing process: Touch-dry in about 10 minutes at 23°C and fully cured in 120 minutes; hot air at 60–80°C can reduce touch-dry time to about 2 minutes.
  • Anti-noise test evidence: VDA 230-206 testing reported no noise for multiple painted-surface, plastic, and leather pairings under the documented conditions.
  • Temperature and emissions data: Documented -40°C to 150°C service range and 0 ppm NMP in VDA 278 thermal-desorption testing.

Applications / Suitable for

  • Door panels, decorative trim, armrests, and related automotive interior interfaces
  • Central consoles, dashboards, glove boxes, clips, and low-load plastic or metal contacts
  • Leather-to-leather, painted-surface-to-leather, and plastic-to-leather interfaces

Technical Specifications

No specifications available.

Additional Information

Water-based air-curing anti-squeak coating

MOLYKOTE® D-96 Anti-Friction Coating

A transparent PTFE-containing dry-film lubricant for controlling squeak and friction in low-load automotive interior contacts. The water-based coating can be sprayed, dip-spun, or brushed onto clean surfaces, then air-cured to provide a thin film for painted-surface, plastic, metal, and leather pairings exposed to slow movement or vibration.

Water-basedPTFE solid lubricantTransparent cured film5–20 µm dry film10 min touch-dry at 23°C-40°C to 150°C
Approved product image showing MOLYKOTE D-96 Anti-Friction Coating packaging and label.

MOLYKOTE® D-96 is supplied as a milky water-based liquid that dries to a transparent anti-friction film.

As supplied

As-supplied coating properties

Coating system
Water-based PTFE
Solid lubricants dispersed in an organic binder, water, and stabilizer.
Application viscosity
41 seconds
Typical DIN EN ISO 2431 flow time at 23°C using a No. 4 cup.
Dry-film appearance
Transparent
Supports friction and noise control without a visible colored coating.
Property Value Unit Method / condition
Dry-film color Transparent — Cured coating
Viscosity at 23°C 41 s DIN EN ISO 2431; No. 4 cup
Density at 23°C 1.33 g/mL ASTM D1475
NMP content 0 ppm VDA 278 thermal-desorption test
Recommended dry-film thickness 5–20 µm Spray, dip-spinning, or brush application
Theoretical coverage at 12 µm Approx. 20 m²/kg Excludes application-process losses

Typical values are not specification limits. Coverage is theoretical and does not include transfer, overspray, drainage, or other application losses.

Application process

Surface preparation, application, and cure

A clean surface, thorough agitation, controlled film build, and sufficient drying time are central to repeatable performance. MOLYKOTE® D-96 is ready to spray and can also be applied by dip-spinning or brushing.

Prepare: Clean and degrease the surface before coating.
Apply: Stir thoroughly, then spray, dip-spin, or brush to a recommended 5–20 µm dry-film thickness.
Dry and cure: Touch-dry after about 10 minutes at 23°C and fully cured after 120 minutes. Hot air at 60–80°C can reduce touch-dry time to about 2 minutes.

 

Stage 1
Clean and degrease
Remove oils, mold release, dust, and other contamination that may interfere with coating wetting or adhesion.
Stage 2
Mix and apply
Stir thoroughly and control the applied quantity to achieve a 5–20 µm dry film by spray, dip-spinning, or brushing.
Stage 3
Dry to handling strength
Allow about 10 minutes at 23°C before handling, or use 60–80°C hot air for an approximately 2-minute touch-dry cycle.
Stage 4
Complete cure and maintain equipment
Allow 120 minutes at 23°C before full loading. Adjust viscosity with distilled or tap water; clean equipment with water or up to 20% DPM or TPM in water.
Storage and handling

Store in the original unopened container at 23°C. The documented usable life is 12 months from the date of production. Review the current safety data and container label before handling, and provide suitable ventilation and eye protection for spray or mist-generating operations.

Performance evidence

Anti-noise and friction performance

The supplier data provide material-pair-specific anti-noise and friction results. These results support evaluation of the listed automotive interior combinations but should not be generalized to untested materials, surface finishes, geometries, loads, temperatures, or vibration profiles.

Anti-noise screening
No noise reported
VDA 230-206 results for eight listed material pairings at 23°C, 40% RH, 2 mm/s, and loads from 2 to 30 N.
Durability evidence
100,000 cycles
No noise reported for 1 mm PVC foil against PC-ABS at 20 N under the stated VDA 230-206 durability conditions.
Service-temperature range
-40°C to 150°C
Documented range for the cured dry film; friction and noise behavior remains application-specific.

VDA 230-206 anti-noise and friction results

Noise screening: 2 mm/s, 23°C, 40% RH, loads 2, 5, 10, 20, and 30 N. Friction coefficients: 2 mm/s, 23°C, 40% RH, 20 N.

Material pairing Noise result Static μ Dynamic μ
Car paint / PVC foil, 1 mm None 0.40 0.27
Car paint / PVC foil, 2.5 mm None 0.29 0.19
Car paint / TPO foil, 1 mm None 0.22 0.13
PVC foil, 1 mm / PVC foil, 1 mm None 0.32 0.21
PC-ABS / PVC foil, 1 mm None 0.31 0.20
Car paint / leather None 0.25 0.19
Leather / leather None 0.29 0.15
PC-ABS / leather None 0.24 0.14

Oscillating-test friction results

Material pairing Static μ Dynamic μ Test condition
POM ball / PVC foil, 1 mm 0.30 0.158 10 mm/s; 2 N; 23°C; 40% RH
POM ball / TPO foil, 1 mm 0.30 0.088 10 mm/s; 2 N; 23°C; 40% RH

All values are typical condition-specific test results, not guaranteed specifications. A low coefficient of friction or a no-noise result in these tests does not establish universal noise elimination, system efficiency, or performance for other material grades and assemblies.

Applications

Automotive interior anti-squeak applications

MOLYKOTE® D-96 is intended for low-load interfaces exposed to slow movement or vibration, particularly where a transparent coating is preferred to a visible lubricant or felt-tape solution. Confirm appearance, adhesion, friction, noise, material compatibility, and durability on the final production assembly.

Automotive door panel and decorative trim interface with a thin transparent anti-squeak coating applied to hidden contact areas.
Door panels, trim, and armrests
Low-load painted-surface, plastic, or metal interfaces in door panels, decorative trim, and armrest assemblies where slow movement or vibration can generate squeak.
Dashboard, center console, and glove-box trim components showing coated hidden contact points between plastic parts and painted surfaces.
Dashboards, consoles, and glove boxes
Plastic-to-plastic, painted-surface-to-plastic, and plastic-to-metal contacts in dashboards, central consoles, glove boxes, clips, and related interior mechanisms.
Automotive leather and plastic trim materials with a transparent coating applied at low-load contact interfaces.
Leather and mixed-material interfaces
Painted-surface-to-leather, plastic-to-leather, and leather-to-leather interfaces where transparent low-friction treatment is needed without changing the visible finish.
Next steps

Evaluate MOLYKOTE® D-96 for your automotive interior interface

Krayden can help review material pairings, surface preparation, application method, target film thickness, drying strategy, appearance requirements, friction targets, and anti-noise validation. Contact us to discuss product fit, sample needs, or a production-representative coating trial.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers