MOLYKOTE D-7409

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

MOLYKOTE D-7409

Main features

  • Heat-Curing Dry-Film Lubricant
  • High-Load Wear-Resistant Dry-Film Lubrication
  • Solvent and Oil Resistance

Product Description

MOLYKOTE® D-7409 Anti-Friction Coating is a high-performance, heat-curing dry-film lubricant formulated with solid lubricants, including molybdenum disulfide and graphite, within an organic binder and solvent system. Designed to replace traditional oils and greases in highly stressed applications, this grayish-black coating provides outstanding permanent lubrication for metal-to-metal combinations operating under moderate to high loads and low sliding speeds.

Key features

  • High load and wear resistance: Withstands extreme contact pressures, exhibiting a Falex load-carrying capacity of up to 11,100 N and excellent endurance on phosphated surfaces.
  • Extreme temperature and chemical stability: Operates reliably across a broad service temperature range of -70°C to 300°C (-94°F to 572°F) while remaining highly resistant to oils, greases, and solvents.
  • Corrosion prevention: Actively avoids fretting corrosion and provides up to 250 hours of protection without red rust in salt spray testing. Formulated without intentional PTFE or PFAS.

Applications / Suitable for

  • Permanent lubrication of highly stressed sliding areas where oils and greases cannot be used
  • Piston rings and tappets of combustion engines
  • Magnetic armatures of vehicle starter motors and bonnet lock components

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Solid lubricants, organic binder, organic solvents - Contains molybdenum disulfide and graphite
Physical State / Appearance Grayish black / Grey - Liquid
Dynamic Viscosity 35 mPas at 23°C (73°F) (ASTM D1084, Method B). SDS reports 400 mPa.s
Kinematic Viscosity 24 mm²/s at 25°C (77°F)
Density 1.1 - 1.17 g/ml at 23°C (73°F) (ASTM D1475). Density values vary slightly between TDS and SDS
Flash Point 40 °C (104°F) Closed cup (ASTM D56)
Boiling Point 138 °C (280°F)
Shelf Life 36 months Stored between 5°C and 23°C in unopened containers from date of production
Technical properties

After-processing / in-service properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Recommended Dry-Film Thickness 5 to 20 µm -
Curing Time 30 minutes at 220°C object temperature
Service Temperature Range -70 to +300 °C (-94 to +572 °F)
Falex Load-Carrying Capacity 8,700 (s) / 11,100 (m) N Procedure B (ASTM D2625) (s=sandblasted, m=Mn-phosphated)
LFW-1 Wear (Oscillating) 158k (s) / 228k (m) / 153k (z) - Oscillations to µ=0.08 (980 N @ 89.5 osc/min) (ASTM D2714) (z=Zn-phosphated)
SRV Load-Carrying Capacity (Ball/Disc) 1,900 (s) / 2,500 (m) / 2,300 (z) MPa Ramp 10 N/3 min, 80 mm/s, 50°C, 40% rel. humidity (ASTM D7217)
SRV Endurance Life (Ball/Disc) > 12 (m) / > 12 (z) h Load 15 N (1,160 MPa), 40 mm/s, 50°C, 40% rel. humidity (DIN 51834)
Corrosion Resistance 250 (z) h Without red rust (steel substrate, 15 µm film) (ASTM B117, DIN 50021)