Main features

  • 700-Hour Cure Cycle
  • 60 to 240 deg C Service Range
  • 60-Minute 180 deg C Cure

Product Description

MOLYKOTE® D-708 Anti-Friction Coating is a black, heat-curing dry-film lubricant for low- to medium-load metal-to-metal and metal-to-plastic interfaces. The PTFE-filled organic binder and solvent system can be spray- or dip-applied after cleaning and degreasing, at a recommended 5–15 µm film thickness, then cured for 60 minutes at 180°C or 20 minutes at 200°C. The cured film operates from -60°C to 240°C and provides a glossy black surface. Typical performance includes a 0.11 coefficient of friction in an internal 50-cycle polymer test, 1,220 N ASTM D2625 Falex pressure resistance, and more than 700 hours of salt-spray resistance for an 11 µm coating over zinc phosphate. Documented uses include safety-belt components, transmission parts, and door locks.

Key features

  • Controlled thin-film process: Apply by spray or dip coating at a recommended 5–15 µm thickness, with documented cure options of 60 minutes at 180°C or 20 minutes at 200°C.
  • Broad cured-film temperature range: Documented operating range of -60°C to 240°C.
  • Condition-specific friction data: Typical coefficient of friction of 0.11 in an internal polymer test using 50 cycles, a 250 g load, and a 20 mm stroke.
  • Corrosion-test evidence: More than 700 hours in an ISO R 1456 salt-spray test for an 11 µm coating applied over zinc phosphate.
  • Glossy black cured finish: Combines lubrication and corrosion-protection functions with a high-quality visible surface finish.

Applications / Suitable for

  • Safety-belt components and related automotive mechanisms
  • Transmission and actuation parts with low- to medium-load sliding contacts
  • Door locks, latches, and closure mechanisms using metal or plastic contact pairs

Technical Specifications

No specifications available.

Additional Information

Heat-curing PTFE dry-film lubricant

MOLYKOTE® D-708 Anti-Friction Coating

A solvent-borne anti-friction coating for low- to medium-load metal-to-metal and metal-to-plastic interfaces. The PTFE solid-lubricant and organic-binder system supports spray or dip application of a controlled thin film, followed by heat cure to create a glossy black lubricating and corrosion-protective surface for automotive and mechanical components.

PTFE solid lubricantOrganic binder / solventSpray or dip application5–15 µm film20 min at 200°C-60°C to 240°C cured film
Approved product image showing MOLYKOTE D-708 Anti-Friction Coating packaging and label.

MOLYKOTE® D-708 is supplied as a black solvent-borne liquid that forms a glossy, heat-cured anti-friction film.

As supplied

As-supplied coating properties

Coating technology
PTFE / organic binder
A dispersion of solid lubricant in an organic resin-solvent system.
Application viscosity
7–10 seconds
Typical ASTM D4212 flow time using a Zahn No. 3 cup.
Density
0.95 g/mL
Typical ASTM D1475 density at 25°C.
Property Value Unit Method / condition
Physical form Liquid — As supplied
Color Black — As supplied
Viscosity 7–10 s ASTM D4212; Zahn No. 3 cup
Density 0.95 g/mL ASTM D1475 at 25°C
Flash point 0 °C ASTM D56

Typical values are not specification limits. The flash-point value describes the as-supplied solvent-borne coating and is not a cured-film operating limit.

Application process

Prepare, coat, and heat cure a controlled thin film

Coating performance depends on surface cleanliness, pretreatment, uniform film build, and a verified cure. Establish process controls using representative components, equipment, and production conditions before fixing the application specification.

Surface preparation: Clean and degrease metal surfaces before application. Zinc-phosphate pretreatment is the substrate condition used for the published salt-spray result.
Application method: Stir well, then apply by spray or dip coating. Adjust application viscosity with methyl ethyl ketone only under the controls required by the current safety information and site procedures.
Target film thickness: Apply a recommended 5–15 µm coating and control the cured film against dimensional and surface-finish requirements.

 

Application sequence and process controls

Stage 1
Clean and prepare
Remove oil, grease, and other contamination from the component. Establish and validate the selected pretreatment, including zinc phosphate where corrosion performance is required.
Stage 2
Mix and apply
Stir the coating thoroughly and apply by spray or dip. Use controlled viscosity, withdrawal or spray settings, and part orientation to obtain uniform coverage.
Stage 3
Control film build
Target a 5–15 µm cured coating. At 10 µm thickness, the documented theoretical coverage is 60 ft²/lb before application losses.
Stage 4
Heat cure and verify
Use 60 minutes at 180°C or 20 minutes at 200°C as documented cure options. Confirm the actual schedule on production-representative parts and ovens.
Storage and handling

Shelf life is 6 months in the original sealed container when stored above -18°C (0°F). The as-supplied coating is highly flammable and has a documented closed-cup flash point of approximately 0°C; review the current safety data and use the required ventilation, ignition-control, grounding, bonding, and personal-protection measures.

Cured-film performance

Cured-film performance and corrosion protection

The cured coating combines friction control, load support, corrosion protection, and a glossy black finish. Interpret each result within its stated film thickness, substrate preparation, test geometry, load, and procedure rather than as a universal assembly limit.

Cured-film temperature range
-60°C to 240°C
Supplier operating guidance for the fully cured dry film.
Coefficient of friction
0.11
Internal polymer test: 50 cycles, 250 g load, and 20 mm stroke.
Salt-spray resistance
>700 h
ISO R 1456 result for an 11 µm coating applied over zinc phosphate.
Property Value Unit Method / condition
Cured-film appearance Glossy black — Visual characteristic of the applied and cured coating
Operating-temperature range -60 to 240 °C Supplier guidance for the cured film
Coefficient of friction 0.11 — Internal polymer test; 50 cycles, 250 g, 20 mm stroke
Falex pressure resistance 1,220 N ASTM D2625
Salt-spray corrosion protection >700 h ISO R 1456; 11 µm coating over zinc phosphate
Theoretical coverage at 10 µm 60 ft²/lb Excludes application-process losses

Typical laboratory results are not guaranteed specifications. The corrosion result applies to the stated 11 µm coating over zinc phosphate, and the coefficient of friction applies only to the identified internal test conditions.

Applications

Automotive and mechanical friction applications

MOLYKOTE® D-708 is intended for low- to medium-load metal-to-metal and metal-to-plastic pairings that can be integrated into a spray- or dip-coating and oven-curing process. Confirm substrate, pretreatment, film thickness, friction target, corrosion requirement, and cure capability on the production assembly.

Automotive safety-belt retractor and buckle components
Safety-belt components
Retractor, buckle, and related mechanisms using low- to medium-load metal-to-metal or metal-to-plastic contacts where a thin cured film can provide friction control, corrosion protection, and a consistent black finish.
Automotive transmission or actuator parts with spray- or dip-applied black anti-friction coating on defined sliding surfaces.
Transmission and actuation parts
Transmission and actuator components that can accommodate cleaning, controlled 5–15 µm film application, and oven cure. Evaluate load, contact material, dimensional tolerance, temperature, and required friction behavior on the actual design.
Door lock
Door locks and closures
Locks, latches, clips, and closure mechanisms with low- to medium-load sliding or contact interfaces where the glossy black cured coating can combine lubrication, corrosion protection, and visible surface finish.
Next steps

Evaluate MOLYKOTE® D-708 for your coated friction component

Krayden can help review contact materials, substrate pretreatment, spray or dip process, target film thickness, cure capability, dimensional tolerance, friction and corrosion requirements, and validation methods. Contact us to discuss product fit, sample needs, or a production-representative coating trial.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers