MOLYKOTE D-321

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE D-321

Main features

  • 5-Minute Cure Cycle
  • 180 to 450 deg C Service Range
  • 12,500 N Falex Load

Product Description

MOLYKOTE® D-321 R Anti-Friction Coating is an air-curing dry-film lubricant available in both bulk liquid and aerosolized spray forms. Formulated with solid lubricants such as molybdenum disulfide and graphite within a solvent and binder system, it provides a gray-black, stick-slip-free coating for metal-to-metal combinations subjected to slow to medium-fast movements and high loads. It cures entirely at room temperature, making it ideal for improving the running-in process and permanently lubricating components like plain bearings, guides, and threaded connections.

Key features

  • Extreme temperature and environment stability: Maintains robust lubrication across a massive service temperature range of -180°C to 450°C and performs exceptionally well even under high vacuum conditions.
  • High load-carrying capacity: Delivers outstanding extreme-pressure protection, with a Falex load-carrying capacity of up to 12,500 N on phosphated surfaces.
  • Convenient air-drying: Becomes touch-dry in just 5 minutes at 23°C and fully cures in 2 hours without the need for high-heat baking.
  • Clean formulation: Features high aging resistance and is formulated without intentional polytetrafluoroethylene (PTFE) or per- and polyfluoroalkyl substances (PFAS).

Applications / Suitable for

  • Lubrication of plain bearings, bushings, sleeves, and power screw drives
  • High voltage switches, slides, guides, and tracks operating at extreme temperatures or in vacuum
  • Emergency boundary lubrication, chains, and hard-to-reach surfaces using the aerosol spray

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Solid lubricants, solvents, binder - Contains molybdenum disulfide and graphite
Physical State / Appearance Gray-black / Black - Bulk liquid or aerosolized spray
Viscosity (Efflux Time) 23 seconds at 23°C (#3 cup, ISO 2431)
Density 1.05 - 1.07 g/ml at 20°C (DIN 53217/2). Value varies between SDS Relative Density and TDS
Nonvolatile Content 29 % CTM 0242 1
Usable Life 24 months Stored between 0 and 40°C in unopened containers from date of production
Technical properties

After-processing / in-service properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Recommended Dry-Film Thickness 5 to 20 µm -
Drying Time (Touch-Dry) 5 minutes at 23°C (can be reduced to 1 minute with 80°C hot air)
Curing Time (Fully Cured) 2 hours at 23°C
Service Temperature Range -180 to 450 °C -
Falex Load-Carrying Capacity 4,500 (b) / 12,500 (p) / 6,800 (s) N ASTM D2625 (b=blank, p=phosphated, s=sandblasted)
LFW-1 Wear (Rotating) 212 (b) / 146 (p) / 306 (s) - Revolutions x 1,000 to µ=0.1 (F=2,860 N, n=72 rpm, v=7.9 m/min) (ASTM D2714)