MOLYKOTE D-10-GBL

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

MOLYKOTE D-10-GBL

Main features

  • 15 to 20 um Dry Film
  • -40 to 340 deg C Service Range
  • 5,500 N Falex Load

Product Description

MOLYKOTE® D-10-GBL Anti-Friction Coating is a gray-black, heat-curing graphite dry-film lubricant for metal-to-metal friction contacts exposed to motor oils, grease, gasoline, diesel, or solvents. The highly viscous coating is formulated for screen printing and may also be sprayed or brushed after viscosity adjustment with gamma-butyrolactone. Recommended processing uses a 15–20 µm dry film, a 10-minute solvent flash-off at 80°C, and a typical 20-minute cure at 200°C object temperature. The cured film has a documented -40°C to 340°C service range and condition-specific Falex and SRV performance data. Applications include engine pistons, compressors, piston pumps, and pneumatic or hydraulic systems.

Key features

  • Graphite dry-film technology: Solid-lubricant coating with an organic binder and solvent carrier for controlled metal-to-metal friction interfaces.
  • Screen-print application: Typical dynamic viscosity of 35,000 mPa·s at 23°C supports screen printing; spraying and brushing are also documented after suitable dilution.
  • Defined film and cure: Recommended 15–20 µm dry-film thickness with a 10-minute flash-off at 80°C and typical 20-minute cure at 200°C object temperature.
  • Fluid-exposure resistance: Documented resistance to oil, grease, gasoline, diesel, and solvents for coated metal contacts.
  • Condition-specific load and wear data: ASTM D2625 Falex load of 5,500 N on manganese-phosphated material and SRV endurance exceeding 12 hours under the stated test conditions.

Applications / Suitable for

  • Gasoline and diesel engine pistons
  • Compressors and piston pumps
  • Pneumatic and hydraulic systems
  • Metal friction contacts exposed to motor oils, fuels, grease, or solvents

Technical Specifications

No specifications available.

Additional Information

Heat-curing graphite dry-film lubricant

MOLYKOTE® D-10-GBL Anti-Friction Coating

A highly viscous, solvent-borne anti-friction coating for prepared metal-to-metal contacts exposed to lubricants, fuels, or solvents. The graphite and organic-binder system supports screen printing of a controlled thin film, followed by solvent flash-off and heat cure for piston, pump, compressor, pneumatic, and hydraulic applications.

Graphite solid lubricantOrganic binder / GBL solvent15–20 µm dry film20 min at 200°CScreen-printable-40°C to 340°C cured film
Approved product image showing MOLYKOTE D-10-GBL Anti-Friction Coating packaging and label.

MOLYKOTE® D-10-GBL is supplied as a gray-black, highly viscous liquid coating that forms a heat-cured graphite dry film.

As supplied

As-supplied coating properties

Coating technology
Graphite / organic binder
The solvent-borne formulation uses graphite solid lubricant in an organic binder system.
Application viscosity
35,000 mPa·s
Typical ASTM D1084 Method B dynamic viscosity at 23°C (73°F).
Density
1.30 g/mL
Typical ASTM D1475 density at 23°C (73°F).
Property Value Unit Method / condition
Color Gray-black — As supplied
Physical form Viscous liquid — Solvent-borne coating
Dynamic viscosity 35,000 mPa·s ASTM D1084 Method B at 23°C (73°F)
Density 1.30 g/mL ASTM D1475 at 23°C (73°F)
Flash point 77 (171) °C (°F) ASTM D56

Typical values are not specification limits. Flash point and uncured-product properties must not be interpreted as cured-film operating limits.

Application process

Prepare, apply, flash off, and heat cure the coating

A controlled surface and cure process is central to coating performance. Clean the substrate, select the pretreatment and application method, maintain the target dry-film thickness, and verify the actual cure on representative production parts.

Surface preparation: Thoroughly clean and degrease the metal surface. Manganese phosphating or 180-grit sandblasting may improve adhesion and coating service life.
Application thickness: Stir thoroughly and target a 15–20 µm dry film. Screen printing is the primary documented method.
Alternative application: Spraying or brushing may be used after adjusting viscosity with gamma-butyrolactone to suit the selected process.

 

Application sequence and process controls

Stage 1
Clean and pretreat
Remove oil, grease, and other contaminants. Use manganese phosphating or 180-grit sandblasting when the application requires enhanced adhesion and service life.
Stage 2
Mix and apply
Stir the coating thoroughly. Apply by screen printing to a recommended 15–20 µm dry-film thickness; spray or brush application requires suitable viscosity adjustment.
Stage 3
Flash off solvent
Before high-temperature cure, use the documented 10-minute flash-off at 80°C (176°F).
Stage 4
Heat cure and validate
A typical schedule is 20 minutes at 200°C (392°F) object temperature. Confirm actual cure for the substrate, part mass, film thickness, and oven design before fixing process specifications.
Storage and handling

Store the original unopened container at or below 23°C (73°F) in a cool, dark location and avoid direct sunlight. Usable life is 12 months from production under these conditions. Review the current safety data and container label before handling, dilution, application, flash-off, or cure.

Cured-film performance

Cured-film performance and operating conditions

The graphite coating is documented for fluid-exposed metal friction contacts and provides condition-specific load, endurance, and friction data. Use these results as evaluation evidence under the stated methods rather than as universal component-load or service-life limits.

Cured-film temperature range
-40°C to 340°C
Documented service-temperature range for the cured dry film; performance remains application- and condition-dependent.
Falex load-carrying result
5,500 N
ASTM D2625 Procedure B on a manganese-phosphated surface.
SRV endurance and friction
>12 h / µ = 0.12
DIN 51834 cylinder/disc result on a sandblasted specimen under the stated load, speed, temperature, humidity, and engine-oil conditions.
Property Value Unit Method / condition
Service-temperature range, cured dry film -40 to 340 (-40 to 644) °C (°F) Supplier service guidance for the cured coating
Falex load-carrying capacity 5,500 N ASTM D2625 Procedure B; manganese-phosphated surface
SRV endurance life >12 h DIN 51834; cylinder/disc, 50 N (150 MPa), 120 mm/s, 50°C, 40% RH, three drops engine oil; sandblasted specimen
SRV coefficient of friction 0.12 µ Same DIN 51834 test conditions
Theoretical coverage at 20 µm Approx. 15 m²/kg Excludes application-process losses

Typical laboratory results are not guaranteed specifications. The service range applies to the cured dry film; bench-test endpoints remain specific to the identified surface preparation, geometry, load, speed, temperature, humidity, lubricant exposure, and duration.

Applications

Piston and fluid-exposed friction applications

The coating is used where a thin, cured graphite film can be integrated into the component manufacturing process. Confirm substrate pretreatment, film thickness, cure, dimensional tolerance, operating fluid, contact pressure, speed, and duty cycle on the actual assembly.

Engine piston and cylinder assembly showing a controlled gray-black dry-film coating on the piston skirt contact area.
Engine pistons
Gasoline and diesel internal-combustion pistons where a thin cured coating is evaluated for break-in, cold-start, and continuing sliding contact with lubricants and fuels.
Compressor with coated piston and cylinder-wall sliding interfaces.
Compressors and piston pumps
Pistons and related sliding metal interfaces in compressors and piston pumps that can accommodate surface preparation, thin-film application, flash-off, and heat cure.
Pneumatic or hydraulic actuator components showing coated metal sliding surfaces exposed to operating fluid.
Pneumatic and hydraulic systems
Metal friction contacts in pneumatic and hydraulic systems, including applications exposed to oils, grease, fuels, or solvents under defined speed and load conditions.
Next steps

Evaluate MOLYKOTE® D-10-GBL for your coated friction interface

Krayden can help review substrate and pretreatment, screen-print or spray process, target film thickness, flash-off and cure capability, dimensional tolerance, operating fluid, load, speed, and validation requirements. Contact us to discuss product fit, sample needs, or a production-representative coating evaluation.