MOLYKOTE BG20

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE BG20

Main features

  • 45 to 180 deg C Service Range
  • 2,400 N Four-Ball Weld Load
  • Manual or Automated Dispensing

Product Description

MOLYKOTE® BG-20 Synthetic Bearing Grease is an NLGI 2–3 polyolester grease thickened with a lithium complex for metal-to-metal bearing contacts operating at high to very high speeds under medium to heavy loads. Its documented service range is -45°C to 180°C, with short periods up to 200°C, and the supplied maximum Dn screening value is 750,000. Typical laboratory data include a 2,400 N four-ball weld load, a 1.0 mm wear scar under 800 N, and an average 662-hour FE9 rolling-bearing result at the stated test condition. It can be applied by brush, spatula, grease gun, automatic device, or central lubrication system.

Key features

  • High-speed bearing capability: Maximum Dn screening value of 750,000; actual suitability varies with temperature, load, and bearing type.
  • Broad temperature range: Service range of -45°C to 180°C, with short periods up to 200°C.
  • Load and wear test data: DIN 51350 four-ball weld load of 2,400 N and 1.0 mm wear scar under an 800 N test load.
  • Low-temperature torque data: ASTM D1478 results are provided at -20°C and -50°C for startup and running evaluation.
  • Flexible application: Suitable for brush, spatula, grease-gun, automatic, and central-system delivery.

Applications / Suitable for

  • Electric motor bearings
  • Blower bearings
  • Calender-roller bearings
  • Clutch-release bearings

Technical Specifications

No specifications available.

Additional Information

High-speed synthetic bearing grease

MOLYKOTE® BG-20 Synthetic Bearing Grease

An NLGI 2–3 polyolester grease with a lithium-complex thickener, anti-wear/extreme-pressure additives, and an oxidation inhibitor. It is intended for metal-to-metal bearings operating at high to very high speeds under medium to heavy loads, including elevated-temperature service.

NLGI 2–3 Polyolester / lithium complex -45°C to 180°C Dn 750,000 55 mm²/s at 40°C
Approved product image showing MOLYKOTE BG-20 Synthetic Bearing Grease packaging and label.

MOLYKOTE® BG-20 is a polyolester-based synthetic grease for high-speed bearing lubrication.

As-supplied grease properties

Lubricant system
Polyolester / lithium complex
Synthetic ester base oil with a lithium-complex thickener, EW/AW additive package, and oxidation inhibitor.
Consistency
NLGI 2–3
ISO 2137 unworked penetration of 240–270 mm/10.
Base-oil viscosity
55 mm²/s
DIN 51562 kinematic base-oil viscosity at 40°C.
Property Value Unit Method / condition
Product form Synthetic bearing grease — Polyolester base oil; lithium-complex thickener
Consistency class 2–3 NLGI Product description
Unworked penetration 240–270 mm/10 ISO 2137
Base-oil viscosity 55 mm²/s DIN 51562 at 40°C
Density 1.01 g/mL ISO 2811 at 20°C
Drop point >295 °C ISO 2176; not an operating-temperature limit

Typical values are not specification limits. NLGI grade, penetration, base-oil viscosity, and drop point describe different characteristics and should not be treated as interchangeable.

Bearing performance and operating limits

Service temperature
-45°C to 180°C
Short-period exposure is listed up to 200°C; this does not imply unchanged grease performance across the full range.
Speed factor
Dn 750,000
Calculated screening value that can vary widely with temperature, load, and bearing type.
FE9 bearing test
662 h average
DIN 51821-02A rolling-element-bearing result at the supplier-listed 1,500/6,000/160°C condition.
Property / test Result Unit Method / condition
Service temperature -45 to 180; up to 200 short term °C Supplier-listed operating range
Initial breakaway torque at -20°C 96 × 10-3 N·m ASTM D1478-07
Running torque after 60 min at -20°C 21 × 10-3 N·m ASTM D1478-07
Initial breakaway torque at -50°C 1,004 × 10-3 N·m ASTM D1478-07
Running torque after 60 min at -50°C 313 × 10-3 N·m ASTM D1478-07
Four-ball weld load 2,400 N DIN 51350 part 4
Wear scar under 800 N 1.0 mm DIN 51350 part 5
Almen-Wieland OK load 20,000 N Frictional force at OK load: 2,250 N
FE9 rolling-element-bearing result 662 average h DIN 51821-02A; supplier notation 1,500/6,000/160°C
Maximum Dn value 750,000 mm/min Calculated approximation; varies with temperature, load, and bearing type
Corrosion rating 1–2 degree DIN 51802 SKF-Emcor method
Oil separation 1.2 % DIN 51817 standard test

These are typical, condition-specific laboratory results. Bench weld-load and wear values are not equipment load ratings, the FE9 result is limited to its stated test condition, and the Dn value does not establish universal bearing speed capability or a relubrication interval.

Application process

Prepare and apply the grease to the bearing system

Use the documented application methods with a clean lubrication point and evaluate the product against the actual bearing type, load, speed, and operating temperature.

Prepare: Clean the points of contact before applying the grease.
Apply: Use a brush, spatula, grease gun, or automatic lubricating device as appropriate for the bearing and maintenance system.
Central delivery: The product is suitable for delivery through a central lubricating system.
Confirm the duty: Treat the temperature range and Dn value as selection inputs; final suitability depends on the specific load, bearing type, speed, and operating environment.

 

Storage and Handling

Store at or below 20°C in the original unopened container. Usable life is 60 months from the date of production. Review current product safety information and the container label before handling.

Applications

High-speed bearing applications

The documented application set centers on metal-to-metal bearings exposed to high speed, medium to heavy loading, and elevated temperature. Product selection should retain the actual bearing geometry, temperature, speed, load, and lubrication-system conditions.

High-speed electric motor bearing installed in an industrial motor assembly.
Electric motor bearings
For electric-motor bearing evaluation, the 750,000 Dn screening value, 55 mm²/s base-oil viscosity at 40°C, and low-temperature torque data provide speed- and startup-related selection inputs.
Industrial blower and calender roller bearing assemblies operating at high rotational speed.
Blower and calender-roller bearings
These documented applications combine rapid motion with industrial temperature and load demands. Evaluate the continuous operating temperature, bearing type, load, and lubrication delivery method together.
Automotive clutch-release bearing positioned within a representative clutch assembly.
Clutch-release bearings
Clutch-release bearings are a documented use context for the grease. Review the actual duty cycle, temperature exposure, rotational speed, load, and grease-delivery requirements before specification.
Next steps

Evaluate MOLYKOTE® BG-20 for your bearing system

Krayden can help review bearing type, rotational speed, Dn calculation, load, continuous and short-term temperature exposure, grease application method, and central-lubrication requirements for electric motors, blowers, calender rollers, clutch-release bearings, and related high-speed mechanisms.

Leading Brands Trust in Our Products and Services