MOLYKOTE BG-555

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE BG-555

Main features

  • Low-Noise Bearing Grease
  • Water-Washout and Corrosion Resistance
  • -40 to 150 deg C Service Range

Product Description

MOLYKOTE® BG 555 Low Noise Grease is a high-performance, wide-temperature-range synthetic grease thickened with lithium soap. Manufactured using a special process in a dust-free environment with strictly selected additives, this light straw-colored grease is expertly formulated to suppress noise and achieve exceptionally quiet bearing performance. The synthetic base oil ensures minimal internal resistance, providing outstanding low-temperature capabilities while maintaining excellent anti-rust properties even in severe moisture or saltwater conditions.

Key features

  • Noise-suppressing performance: Purified raw materials and controlled manufacturing yield a Class II/1 rating in the FAG MGG-11 low-noise performance test.
  • Extended service life: Highly oxidation-resistant and thermally stable, providing a significantly longer performance life (4,000 hours at 125°C) than conventional wide-temperature lithium greases.
  • Wide temperature capability: Functions reliably from -40°C to +150°C (-40°F to 302°F), facilitating easy cold starting for precision machinery and small motors.

Applications / Suitable for

  • Rolling element bearings requiring low noise and long operational life at elevated temperatures
  • Precision machines and small size electric motors requiring low starting torque
  • Automotive electric equipment operating in severe environmental conditions (e.g., saltwater)

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Synthetic lubricating oils, lithium 12-hydroxyoctadecanoate soap - -
Appearance / Color Light straw / Light yellow - Grease
Base Oil Kinematic Viscosity 26.0 mm²/s at 40°C (104°F) (ASTM 445)
Worked Penetration 255 mm/10 ASTM D217
Relative Density 1.0 - Water = 1
Flash Point 225 °C Closed cup (437°F)
Shelf Life 36 months When stored at or below 40°C (104°F) from the date of production
Technical properties

After-processing / in-service properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Service Temperature Range -40 to +150 °C (-40 to +302 °F)
Dropping Point 195 °C (383°F) (ASTM D566)
Working Stability 315 mm/10 FTM 791C-313
Water Washout 1.3 mass % 1 hour at 38°C (100.4°F) (ASTM D1264)
Low-Temperature Torque (Starting) 15 N.cm at -40°C (-40°F) (ASTM D1478-63)
Low-Temperature Torque (Running) 3.0 N.cm at -40°C (-40°F) (ASTM D1478-63)
Evaporation Loss 0.30 mass % 22 hours at 99°C (210.2°F) (ASTM D972)
Oil Separation 1.0 mass % 24 hours at 100°C (212°F) (FTM 791C-321 Mod)
Oxidation Stability 2.5 kPa ASTM D942
Copper Strip Corrosion 1a - 24 hours at 100°C (212°F) (ASTM D4048)
Corrosion Preventive Properties 1 - 48 hours at 52°C (125.6°F) (ASTM D1743-73)
SKF-Emcor Method Degree of Corrosion 0-0 - DIN 51 802
Low-Noise Performance Test Class II/1 - FAG MGG-11
DN Value 1,300,000 mm/min Calculated approximation (varies with temperature, load, bearing type)
Life Performance 4,000 hour at 125°C (257°F) (ASTM D1741)

Leading Brands Trust in Our Products and Services