MOLYKOTE 557

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

MOLYKOTE 557

Main features

  • Clear Nonstaining Wax-Like Film
  • 0.07 Coefficient of Friction
  • Federal Meat/Poultry Program Authorization

Product Description

MOLYKOTE® 557 Silicone Dry Film Lubricant is an extreme-pressure, wax-like dry-film lubricant supplied in a solvent carrier (available as a bulk liquid or aerosol spray). Once applied, the solvent evaporates to leave a nearly transparent, clear wax film that adheres tenaciously to surfaces in both solid and fluid states. It provides exceptional release properties and heavy-duty lubrication, effectively reducing friction, wear, stick-slip, and metal seizure in demanding manufacturing and metalworking operations.

Key features

  • Clean and nonstaining: Dries to a colorless film that will not stain paper or fabrics, and is formulated without intentional polytetrafluoroethylene (PTFE) or per- and polyfluoroalkyl substances (PFAS).
  • Extreme-pressure performance: Protects heavily loaded tracks, cams, slides, and cutting tools with a four-ball weld load capacity of 1,200 N.
  • Industry authorized: Authorized for use in official establishments operating under the Federal Meat and Poultry Inspection Program (formerly USDA H2 ratings) where there is no possibility of food contact.

Applications / Suitable for

  • Metalworking operations: extruding, deep drawing, spinning, and increasing the life of slitter-blades, taps, dies, and drills
  • Lubricating heavily loaded bearings, slides, cams, adjusting screws, guides, and ways in machine shops
  • Reducing sticking and product contamination on conveyors, knives, and handling equipment in the textile, paper, woodworking, rubber, and plastic industries

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Waxlike lubricant in solvent carrier - Bulk solvent is naphtha
Appearance / Color Clear / Colourless - Supplied as liquid or aerosol spray
Specific Gravity (Bulk Liquid) 0.77 - CTM 0137A
Relative Density (Aerosol) 0.8 - Water = 1
Flash Point (Bulk Liquid) 39 °C (102°F) Bulk form only
Drying Time 30 minutes -
Usable Life (Bulk Liquid) 60 months Stored at or below 25°C (77°F) from date of manufacture
Usable Life (Aerosol Spray) 24 months Stored at or below 25°C (77°F) from date of manufacture
Technical properties

After-processing / in-service properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Appearance (As Applied) Clear wax film - After solvent evaporation
Service Temperature Range -40 to 43 °C (-40 to 110 °F) Estimated based on formulation
Melting Range 32 to 46 °C (90 to 115 °F)
Coefficient of Friction 0.07 - Tested on Falex LFW-4 Press Fit tester, steel vs. steel
Press Fit Performance No stick-slip - Falex LFW-4 Press Fit tester, steel vs. steel, Rc60, 12,000 psi
Four Ball Weld Load 1,200 N ASTM D2596
Four Ball Wear Scar 0.85 mm Fed Std 791a, Method 6514.1