MOLYKOTE 55

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE 55

Main features

  • Silicone Base Oil and Lithium Soap Thickener
  • Heat-Stable Oxidation-Resistant Grease
  • D4/D5/D6 Cyclic-Siloxane Compliance

Product Description

MOLYKOTE® 55 O-Ring (S) Grease is a beige silicone-based grease formulated with silicone oil, ester oil, and lithium soap for lubricating rubber-to-metal O-ring and seal interfaces in pneumatic systems. The documented service range is -65°C to +175°C, with ASTM D1478-80 low-temperature torque data measured at -65°C. Typical retention data include less than 1% evaporation and less than 7% bleed after 24 hours at 150°C, plus 3% oil separation after 7 days at 40°C. The formulation is designed to slightly swell compatible rubber O-rings and seals while supporting lubrication and sealing. For ultra-low cyclic silicone lubricant programs, it complies with the limits on cyclic siloxanes (D4, D5 and D6) in accordance with Regulation (EU) 2024/1328. Material response can vary with elastomer formulation and plasticizer content, so small-scale compatibility testing should be conducted before use in a specific assembly.

Key features

  • Wide service-temperature range: Documented for approximately -65°C to +175°C service.
  • Low-temperature torque data: 115 × 10-3 N·m initial breakaway torque and 21 × 10-3 N·m after 20 minutes at -65°C.
  • Condition-specific evaporation data: Less than 1% evaporation after 24 hours at 150°C; this is a measured retention result, not a universal outgassing or low-fogging qualification.
  • Ultra-low cyclic regulatory positioning: Complies with the limits on cyclic siloxanes D4, D5 and D6 in accordance with Regulation (EU) 2024/1328.
  • Water and corrosion test data: Static water-resistance rating 0-90 at 90°C for 3 hours, 5.2% ASTM D1264 water washout, and SKF-EMCOR corrosion degree 0.
  • Application flexibility: Apply by brush, grease gun, automatic lubrication equipment, or centralized lubrication system; do not mix with other greases.
  • Compatibility control: Intended for elastomer-containing interfaces, with small-scale material compatibility testing required for the exact seal or polymer grade.

Applications / Suitable for

  • Rubber-to-metal O-rings and seals in pneumatic systems
  • Aircraft pneumatic-system O-ring and seal lubrication
  • Automotive pneumatic-system O-ring and seal lubrication
  • General industrial pneumatic-system O-ring and seal lubrication

Technical Specifications

No specifications available.

Additional Information

Silicone-based O-ring grease for pneumatic systems

MOLYKOTE® 55 O-Ring (S) Grease

A beige silicone-based grease using silicone oil, ester oil, and lithium soap for rubber-to-metal O-ring and seal interfaces in aircraft, automotive, and general industrial pneumatic systems. It provides a -65°C to +175°C service range, low-temperature torque and retention data, and controlled material-compatibility guidance. For ultra-low cyclic silicone lubricant programs, it complies with the limits on cyclic siloxanes D4, D5 and D6 in accordance with Regulation (EU) 2024/1328.

-65°C to +175°C Silicone + ester oil Lithium soap thickener <1% evaporation at 150°C / 24 h O-ring and seal lubrication
MOLYKOTE 55 O-Ring (S) Grease package and label.

MOLYKOTE® 55 O-Ring (S) Grease is a beige silicone-based grease for O-ring and seal lubrication.

As supplied

Grease composition, consistency, and physical properties

Grease system
Silicone / ester / lithium soap
Silicone oil and ester oil thickened with lithium soap.
Base-oil viscosity
100 mm²/s
DIN 51562 kinematic base-oil viscosity at 25°C.
Worked penetration
260–300 mm/10
ISO 2137 consistency result; penetration is not the same property as base-oil viscosity.
Property Value Unit Method / condition
Color Beige — As supplied
Kinematic base-oil viscosity 100 mm²/s DIN 51562; 25°C
Worked penetration 260–300 mm/10 ISO 2137
Density 0.98 g/cm³ ISO 2811; 25°C
Dropping point ≥195 °C ASTM D2265; test transition, not the service-temperature limit

Supplier data are identified as preliminary and typical; they are not specification limits. Base-oil viscosity, penetration, and dropping point describe different properties and should not be treated as interchangeable service limits.

In service

Temperature, retention, and in-service test results

The results below are condition-specific evaluation data. Evaporation, bleed, oil separation, oxidation, friction, water resistance, washout, and corrosion are different measurements; none should be converted into a universal low-outgassing, contamination-free, maintenance-life, or system-reliability claim.

Ultra-low cyclic and regulatory context
For ultra-low cyclic silicone lubricant programs, MOLYKOTE® 55 O-Ring (S) Grease complies with the limits on cyclic siloxanes D4, D5 and D6 in accordance with Regulation (EU) 2024/1328. This regulatory statement is specific to the cited cyclic-siloxane limits; low-fogging, low-outgassing, lubricant-migration, sensor, optics, and assembly-cleanliness requirements should still be qualified separately when they apply.
Service range
-65°C to +175°C
Documented approximate service-temperature range.
Evaporation
<1%
ASTM D6184 after 24 hours at 150°C.
Low-temperature torque
115 / 21 mN·m
ASTM D1478-80 at -65°C: initial breakaway / after 20 minutes.
Property Value Unit Method / condition
Service temperature -65 to +175 °C Approximate product service range
Initial breakaway torque 115 × 10-3 N·m ASTM D1478-80; -65°C
Torque after 20 min 21 × 10-3 N·m ASTM D1478-80; -65°C, after 20 min
Bleed <7 % ASTM D6184; 150°C / 24 h
Evaporation <1 % ASTM D6184; 150°C / 24 h
Oil separation 3 % DIN 51817; 40°C / 7 days
Oxidation pressure loss ≤100 mbar DIN 51808; 100 h at 99°C
RapidOxy 100 oxidation stability 900 min DIN 51830-1; accelerated procedure at 160°C
Coefficient of friction 0.02 µ Steel ball / POM; 12.7 mm ball, 6.3 N, 10 mm/s, 24 h
Static water resistance 0-90 rating DIN 51807 part 1; 90°C / 3 h
Water washout 5.2 % ASTM D1264
Corrosion degree 0 rating DIN 51802; SKF-EMCOR method

Use the evaporation result as the measured ASTM D6184 value at 150°C for 24 hours. It does not establish low-fogging, low-outgassing, vacuum suitability, lubricant-migration limits, or sensor/optics compatibility without application-specific evidence.

Application process

Apply to a verified O-ring or seal material and avoid lubricant mixing

The grease may be applied by brush, grease gun, automatic lubrication equipment, or centralized lubrication systems. Because the formulation is intended to interact with elastomer seals, material compatibility is a selection step rather than an assumed property of every rubber or plastic grade.

Compatibility check: Conduct small-scale testing on the exact material before use; lubricant response can vary with elastomer formulation and plasticizer content.
Restricted materials: Do not use with silicone rubber, polycarbonate, or ABS unless the specific application has been thoroughly tested.
Lubricant mixing: Do not mix with other greases.
Technician applying a controlled amount of grease to a rubber O-ring before assembly with a metal pneumatic-system component.

Use the final processing visual to show controlled O-ring or seal lubrication at a rubber-to-metal pneumatic interface.

Stage 1
Verify the interface
Confirm the O-ring or seal material, mating metal, temperature range, pneumatic duty, cyclic-siloxane requirements, and any low-fogging, outgassing, migration, or contamination-control targets before specification.
Stage 2
Run compatibility testing
Use a small-scale material test when the elastomer or polymer response has not already been validated for the specific assembly.
Stage 3
Apply with the selected method
Apply by brush, grease gun, automatic lubrication system, or centralized lubrication system according to the assembly and process design.
Stage 4
Keep the grease system controlled
Do not mix with other greases. Where contamination or migration is critical, validate the complete assembled system rather than relying on a single evaporation or separation result.
Storage and handling

Store between 0°C and 40°C in the original unopened container. Usable life is 60 months from the date of production. Review the current safety information and container label before handling. Do not use with liquid oxygen or other strong oxidizers.

Applications

O-ring and pneumatic-system applications

The documented application scope is lubrication between rubber and metal parts in pneumatic systems. For other contamination-sensitive assemblies, qualify the exact interface, material pair, operating conditions, and cleanliness requirement before treating the grease as a suitable solution.

Aircraft pneumatic-system O-ring and metal fitting shown as a representative lubrication interface.
Aircraft pneumatic O-rings and seals
Documented application context for rubber-to-metal lubrication in aircraft pneumatic systems. Validate the exact elastomer formulation, temperature exposure, pressure cycle, and assembly requirements.
Automotive pneumatic actuator or valve assembly with a rubber O-ring at a metal interface.
Automotive pneumatic O-ring interfaces
Applicable to the documented automotive pneumatic-system use where lubrication is required between rubber seals and metal components. Confirm compatibility for the exact seal grade and lubricant exposure.
Industrial pneumatic cylinder, valve, or fitting with a rubber O-ring and metal sealing surface.
General industrial pneumatic systems
General industrial pneumatic O-ring and seal interfaces are within the documented application scope. Evaluate operating temperature, water exposure, material grade, grease quantity, and any cleanliness requirements at assembly level.
Next steps

Evaluate MOLYKOTE® 55 O-Ring (S) Grease for your seal interface

Krayden can help review the O-ring or seal material, mating surface, pneumatic duty, temperature range, lubricant quantity, application method, cyclic-siloxane limits, and contamination-control requirements. For ultra-low cyclic programs or applications involving sensors, optics, or electronics, qualify any low-fogging, outgassing, migration, and assembly-cleanliness targets separately.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers