MOLYKOTE 5

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE 5

Main features

  • Nonconductive, Water-Repellent Silicone Paste
  • 54 to 232 deg C Service Range
  • Metal and Plastic Compatibility

Product Description

MOLYKOTE® 5 Compound is a nonconductive, water-repellent silicone paste engineered primarily for use as a dielectric compound on insulators, bushings, and high-current switches. Formulated with an inert amorphous silica filler and selected dimethyl and phenylmethyl silicone fluids, it provides improved metal-to-metal lubricity compared to standard silicone compounds. This virtually inert and nonvolatile grease-like material effectively prevents the formation of conductive paths, arcing, and flashovers on high-voltage equipment while resisting oxidation and moisture.

Key features

  • Broad operating range: Delivers a serviceable temperature range of -54 to 232°C (-65 to 450°F), representing a significant improvement over traditional silicone compounds.
  • Excellent material compatibility: Highly compatible with rubber, metal, and plastic components, making it ideal for lubricating static and dynamic O-ring seals.
  • Clean and compliant: Formulated without intentional polytetrafluoroethylene (PTFE) or per- and polyfluoroalkyl substances (PFAS).

Applications / Suitable for

  • Preventing arcing and flashovers on insulators, bushings, and high-voltage equipment contacts
  • Lubricating static and dynamic O-ring seals in hot-melt adhesive equipment
  • Water-repellent filling material for service entrance cable jackets
  • Preventing rust, oxidation, and corrosion on insulator threads, bolts, and watt-hour meter contacts

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Dimethyl and phenylmethyl silicone fluids, amorphous silica filler - Silicone paste
Physical State / Appearance Light gray to translucent white - Grease
Unworked Penetration 170-230 mm/10 ASTM D217
Relative Density 1 - Water = 1
Flash Point > 101.1 °C Closed cup (> 214.0 °F)
Shelf Life 60 months From date of manufacture
Technical properties

After-processing / in-service properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Service Temperature Range -54 to 232 °C (-65 to 450 °F)
Worked Penetration 228 mm/10 Worked 60 strokes, 1/2 scale (ASTM D1403)
Bleed 0.4 % 30 hours at 204°C (399°F) (AMS8660)
Evaporation 1.2 % 30 hours at 204°C (399°F) (AMS8660)
Volume Change Rubber -0.6 % SRE-NBR-28/PX (ASTM D471, AMS8660)
Durometer Hardness Change +2 - Delta (80 Shore A) (ASTM D2240)
Low Temp Torque (Starting) 2087 gm-cm at -54°C (-65°F) (ASTM D1478)
Low Temp Torque (Running) 313 gm-cm at -54°C (-65°F), 60 minutes (ASTM D1478)
Dielectric Strength 321 volts/mil 50 mil gap (ASTM D149, AMS8660)
Volume Resistivity 1.61x10^14 ohm-cm at 23°C 500VDC (ASTM D257, AMS8660)
Volume Resistivity 1.51x10^14 ohm-cm at 177°C 500VDC (ASTM D257, AMS8660)
Arc Resistance 124 seconds mean (ASTM D495, AMS8660)
Dielectric Constant 2.77 / 2.91 / 2.76 - at 1 kHz / 1 MHz / 10 MHz (ASTM D150, AMS8660)
Dissipation Factor 0.0004 / 0.0017 / 0.0026 - at 1 kHz / 1 MHz / 10 MHz (ASTM D150, AMS8660)
Thermal Conductivity 0.238 W/mK at 30°C (ASTM D5470)
Specific Heat 1.385 / 1.502 / 1.541 J/(g°C) at 50°C / 100°C / 150°C (ASTM E2716)