MOLYKOTE 44

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE 44

Main features

  • -40 to 200 deg C Service Range
  • 2.5% Bleed at 150 deg C
  • NLGI 2-3 Silicone Grease

Product Description

MOLYKOTE® 44 Medium High Temperature Grease is a white-to-off-white, NLGI 2–3 silicone-oil grease thickened with lithium soap for bearings and other lubricated contacts across a documented -40°C to 200°C service range. Its 125 mm²/s base-oil viscosity at 25°C, 240–280 mm/10 worked penetration, and maximum Dn value of 300,000 support evaluation across different bearing speeds and application methods. Typical retention data include 2.5% bleed and 2.0% evaporation after 24 hours at 150°C, while water washout is 1.0% at 38°C. Applications include oven-fan, textile-dryer, conveyor, kiln-preheater, and automotive clutch-release bearings, as well as selected plastic parts.

Key features

  • Broad operating range: Documented service temperature range of -40°C to 200°C for high-temperature and general bearing evaluation.
  • Controlled grease consistency: NLGI 2–3 with 240–280 mm/10 worked penetration and a 125 mm²/s silicone base oil at 25°C.
  • High-temperature retention data: Typical bleed of 2.5% and evaporation of 2.0% after 24 hours at 150°C.
  • Oxidation and water-resistance data: DIN 51808 pressure loss of ≤100 mbar after 100 hours at 99°C and 1.0% water washout at 38°C.
  • Flexible application: Apply to clean lubrication points by brush, spatula, or automatic lubrication equipment.

Applications / Suitable for

  • Oven-fan and textile-dryer bearings
  • Conveyor and kiln-preheater bearings
  • Automotive clutch-release bearings
  • Selected plastic parts, subject to material-specific validation

Technical Specifications

No specifications available.

Additional Information

High-temperature bearing grease

MOLYKOTE® 44 Medium High Temperature Grease

A white-to-off-white, lithium-thickened silicone grease for bearings and selected plastic parts across a documented -40°C to 200°C service range. NLGI 2–3 consistency, a 125 mm²/s base-oil viscosity at 25°C, and controlled bleed, evaporation, oxidation, and water-washout data support application-specific evaluation.

NLGI 2–3 -40°C to 200°C Silicone oil / lithium soap 125 mm²/s at 25°C Water-resistant
MOLYKOTE 44 Medium High Temperature Grease

MOLYKOTE® 44 Medium is supplied as a white-to-off-white silicone grease with NLGI 2–3 consistency.

As-supplied grease properties

Lubricant system
Silicone oil / lithium soap
White-to-off-white grease with NLGI 2–3 consistency.
Consistency and base oil
240–280 mm/10
CTM0190 worked penetration after 60 strokes; base-oil viscosity is 125 mm²/s at 25°C.
Density
1.0 g/cm³
Typical density for the as-supplied grease.
Property Value Unit Method / condition
Appearance White to off-white — As supplied
Base oil / thickener Silicone oil / lithium soap — Product composition
Base-oil viscosity 125 mm²/s Kinematic viscosity at 25°C
Worked penetration 240–280 mm/10 CTM0190; 60 strokes
NLGI class 2–3 — Consistency classification
Density 1.0 g/cm³ Typical value

Typical values are not specification limits.

Temperature and retention properties

Service temperature
-40°C to 200°C
Documented service range; validate bearing design, load, speed, and relubrication conditions at the intended operating point.
Maximum Dn estimate
300,000
Selection input based on bearing bore in millimeters multiplied by rotational speed; not an equipment-capacity guarantee.
High-temperature retention
2.0% evaporation
ASTM D6184 result after 24 hours at 150°C; bleed under the same condition is 2.5%.
Property Value Unit Method / condition
Service temperature range -40 to 200 °C Documented product range
Drop point 227 °C IP 396/02
Bleed 2.5 % ASTM D6184; 150°C for 24 hours
Evaporation 2.0 % ASTM D6184; 150°C for 24 hours
Oxidative stability ≤100 (≤0.01) mbar (MPa) DIN 51808; pressure loss after 100 hours at 99°C
Water washout 1.0 % DIN 51807, part 2; 38°C
Maximum Dn value 300,000 mm/minute Supplier-reported bearing-speed selection value

Drop point is a test transition and is not the maximum continuous operating temperature. All values are typical and should be evaluated under the intended bearing and service conditions.

Application process

Prepare and apply the grease to clean lubrication points

Application is straightforward, but grease quantity, delivery method, component materials, and existing lubricant condition should be reviewed for the specific bearing or mechanism.

Prepare: Clean the lubrication point before applying or filling the grease.
Apply: Use a brush, spatula, or automatic lubrication device according to the component geometry and maintenance system.
Validate materials: The product is described as compatible with most plastics, but confirm the exact polymer grade, exposure temperature, and existing lubricant combination.
Observe the limitation: Do not use on painted surfaces.

 

Storage and Handling

Store unopened in a cool, dark place. Usable life is 60 months from the date of production. Review current product safety information and the container label before handling.

Applications

High-temperature bearing applications

Documented applications center on bearings exposed to elevated temperature or broad operating-temperature changes. Final suitability depends on bearing design, speed, load, materials, grease quantity, and relubrication practice.

Oven fan or textile dryer bearing installed near a high-temperature air-handling assembly.
Oven-fan and textile-dryer bearings
These applications place bearings near sustained heat and airflow. Use the documented temperature range, evaporation, bleed, oxidation, and bearing-speed inputs to define an equipment-specific lubrication plan.
Conveyor or kiln preheater bearing in an industrial high-temperature processing line.
Conveyors and kiln preheaters
Documented use includes conveyor and kiln-preheater bearings. Evaluate the actual bearing temperature, environmental contamination, water exposure, speed, and relubrication access before selection.
Automotive clutch-release bearing beside a representative molded plastic component.
Clutch-release bearings and plastic parts
Applications also include automotive clutch-release bearings and selected plastic parts. Confirm the specific polymer, contact geometry, duty cycle, and lubrication requirements through end-use testing.
Next steps

Evaluate MOLYKOTE® 44 Medium for your bearing application

Krayden can help review bearing type, load, speed, temperature, plastics compatibility, grease quantity, application method, and relubrication requirements for oven fans, dryers, conveyors, kiln equipment, automotive bearings, and related mechanisms. Contact us to discuss product fit, samples, or an application-specific evaluation plan.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers