MOLYKOTE 3099

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE 3099

Main features

  • Water-Repellent High-Voltage Insulator Coating
  • 800-Minute ASTM D2303 Arc Resistance
  • Hand, Pad, Brush, or Spray Renewal

Product Description

MOLYKOTE® 3099 HVIC Compound is a gray, opaque, greaselike silicone protective coating for high-voltage electrical insulators. It combines water repellency with arc resistance to support flashover protection under high-voltage stress, ultraviolet exposure, water erosion, and particulate contamination. The soft, non-stringy compound adheres to properly prepared insulators and can be applied by hand, cloth pad, bristle brush, or properly configured airless spray equipment. Its opaque color supports visual confirmation of a smooth, complete coating, while typical electrical data include 1.46 × 1013 ohm-cm volume resistivity and 285 V/mil dielectric strength at 50 mil thickness. Normal application produces a 1/16- to 1/8-in coating; the exact service interval remains site-dependent and should be established through inspection and operating experience.

Key features

  • Water-repellent protective coating: Grease-like silicone formulation for electrical insulators exposed to high-voltage stress, ultraviolet light, water erosion, and particulate contamination.
  • Arc resistance: Typical ASTM D2303 result of 800 minutes to erode a 1/8-in coating at 2.5 kV.
  • Electrical properties: Typical volume resistivity of 1.46 × 1013 ohm-cm and dielectric strength of 285 V/mil at 50 mil thickness, ASTM D149.
  • Controlled application: Applies by hand, cloth pad, bristle brush, or properly configured airless spray equipment at a typical thickness of 1/16 to 1/8 in.
  • Visual coverage control: Gray, opaque appearance helps operators confirm a smooth, complete coating on prepared insulator surfaces.

Applications / Suitable for

  • High-voltage transmission-line insulator strings
  • Suspension insulators in coastal or contamination-exposed installations
  • Substation bushings and related high-voltage electrical insulators

Technical Specifications

No specifications available.

Additional Information

Electrical insulator protective coating

MOLYKOTE® 3099 HVIC Compound

A gray, greaselike silicone coating for electrical insulators exposed to high-voltage stress. Water repellency, arc-resistant formulation, good adhesion, and a soft, non-stringy consistency support uniform application and evaluation in ultraviolet, water-erosion, and particulate-contamination environments. The coating remains soft for removal and recoating, while its gray opacity supports visual coverage checks.

Grease-like silicone coating Gray opaque appearance Arc- and flashover-resistant 100% solids Hand, brush, pad, or spray
MOLYKOTE 3099 HVIC Compound

MOLYKOTE® 3099 HVIC Compound is supplied as a gray, greaselike silicone coating for electrical insulators.

As-supplied compound properties

Physical form
Grease-like silicone compound
Soft, non-stringy consistency supports spreading and coating of properly prepared insulator surfaces.
Appearance and solids
Gray opaque / 100% solids
Opaque color supports visual coverage checks; the listed solids value is a typical CTM 0208 result.
Property Value Unit Method / condition
Appearance Gray opaque — As supplied
Consistency, unworked penetration 260 — ASTM D127
Consistency, worked penetration 270 — ASTM D127
Specific gravity 1.3 — CTM 0001A at 77°F (25°C)
Solids 100 % CTM 0208
Flash point, closed cup >250 (>121) °F (°C) CTM 0006

Typical values are not specification limits.

Applied coating electrical properties

Arc resistance
800 min
Typical ASTM D2303 time to erode a 1/8-in coating at 2.5 kV; the result is specific to the stated test conditions.
Volume resistivity
1.46 × 1013 ohm-cm
Typical ASTM D149 bulk resistivity value for the tested material.
Property Value Unit Method / condition
Dielectric constant 3.88 — ASTM D150 at 100 Hz
Dielectric constant 3.86 — ASTM D150 at 1,000 Hz
Dissipation factor 0.0148 — ASTM D150 at 100 Hz
Dissipation factor 0.0066 — ASTM D150 at 1,000 Hz
Volume resistivity 1.46 × 1013 ohm-cm ASTM D149
Dielectric strength 285 V/mil ASTM D149; 50 mil specimen thickness
Arc resistance 800 min ASTM D2303; time to erode a 1/8-in coating at 2.5 kV

These are typical laboratory values, not guaranteed specifications or universal system-performance limits. Evaluate the coating under the intended end-use conditions before specification.

Application process

Prepare, apply, and maintain a complete coating

Application quality depends on a clean, dry insulator surface and a smooth, continuous coating. Select hand, pad, brush, or airless-spray application according to the insulator geometry and site conditions.

Surface condition: Remove dirt, organic residues, and cleaning detergents; allow the insulator to dry completely before coating.
Target thickness: Normal hand or spray application produces approximately 1/16 to 1/8 in; use 1/8 in for the most severely contaminated conditions.
Application methods: Apply by hand, cloth pad, bristle brush, or properly diluted airless spray equipment.
Technician applying a smooth gray silicone coating to high-voltage insulator skirts, treating the underside before working down the stack.

Application should create smooth, complete coverage while avoiding overfill between the underside skirts of fog-type insulators.

Application sequence and equipment guidance

Stage 1
Clean and dry the insulator
Clean the full surface, remove traces of organics or detergent, and confirm the insulator is dry before application.
Stage 2
Apply from the top downward
Treat the underside of the top insulator first and work down the stack. Build a smooth, complete 1/16- to 1/8-in coating and avoid overfilling fog-type skirts.
Stage 3
Configure airless spray when needed
Use approximately 70% compound and 30% appropriate solvent as a starting blend. Mix thoroughly; use a pump compression ratio of at least 26:1, a 0.013- to 0.026-in nozzle, with 40-60 psi for larger-orifice nozzles and 60-80 psi for smaller-orifice nozzles.
Stage 4
Inspect, remove, and recoat
Establish site-specific inspection intervals. Check the gray coating for visible paths of decomposition; when renewal is required, wipe the soft coating away with coarse-textured rags or paper towels and apply a new coat.
Storage and Handling

Shelf life is 60 months from the date of manufacture. Review the current safety data and container label before handling. When spraying or using a solvent, follow the solvent supplier’s safety recommendations and applicable regulations. Do not use flammable or combustible solvents for application to energized circuits.

Applications

Electrical insulator application contexts

The compound is used as a protective coating on electrical insulators. Use and field-test contexts include transmission, coastal suspension, and substation installations; product fit and service intervals remain specific to the insulator design, contamination level, electrical stress, and maintenance practice.

High-voltage transmission tower with a clearly visible suspension insulator string.
Transmission-line insulator strings
Applied as a continuous protective coating on high-voltage transmission insulators where water filming, ultraviolet exposure, particulate contamination, and corona stress are important evaluation factors.
Coastal suspension insulator string in an outdoor high-voltage installation.
Coastal and contamination-exposed suspension insulators
Relevant for suspension strings evaluated in coastal or heavily contaminated environments. Water repellency, arc resistance, complete skirt coverage, and a site-specific inspection plan are central selection considerations.
High-voltage substation bushing installed on electrical equipment.
Substation bushings
Used on bushings and related substation insulators where a visible gray coating can support coverage checks and inspection for paths of decomposition before removal and recoating.
Next steps

Evaluate MOLYKOTE® 3099 HVIC Compound for your insulator system

Krayden can help review insulator geometry, contamination severity, application method, target coating thickness, airless-spray setup, and inspection strategy. Contact us to discuss product selection, sample needs, technical data interpretation, or a site-specific evaluation plan for transmission and substation insulation.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers