Main features

  • High-Viscosity Lubricant Formulation
  • Robust High-Pressure Resistance and Wear Protection
  • High-Temperature Lubrication Protection

Product Description

MOLYKOTE® 1122 Chain and Open Gear Grease is a high-performance synthetic grease formulated with a very high viscosity base oil (1,500 mm²/s at 40°C), an inorganic thickener, solid lubricants, and a specialized adhesion improver. Designed to be extremely adhesive and water-resistant, this black paste excels in lubricating slow-moving, heavily loaded sliding bearings, open gears, and chains equipped with hollow pins. It contains no intentional PTFE or PFAS and is engineered to provide emergency lubrication and exceptional wear protection under extreme pressures.

Key features

  • Extreme adhesion and water resistance: The specialized adhesion improver ensures the grease remains precisely where applied, providing robust resistance against water washout in challenging environments.
  • High load and wear protection: Exhibits a high four-ball weld load of 2,600 N and an Almen Wieland OK load of 18,000 N, offering superb high-pressure resistance and emergency lubrication.
  • Reliable operation at elevated temperatures: Maintains strong lubricating properties over a service temperature range of 10°C to 160°C.

Applications / Suitable for

  • Initial and ongoing lubrication of chains with hollow pins equipped with grease nipples, such as tenter clamp chains and food sterilizer conveyor chains
  • Open gears and gear drives
  • Sliding bearings operating at low speeds and high temperatures (e.g., drying systems, calendering machines)

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Synthetic oil, solid lubricants, inorganic thickener, adhesion improver - Contains molybdenum sulfide, graphite, and talc
Physical State / Appearance Black - Paste
Base Oil Viscosity 1,500 mm²/s at 40°C
Unworked Penetration 250-280 - -
Density 0.95 g/ml at 20°C
Flash Point > 200 °C Pensky-Martens closed cup
Usable Life (Paste/Grease) 60 months Stored at or below 20°C in unopened containers
Usable Life (Aerosol Spray) 24 months Stored between 5°C and 35°C in unopened containers
Technical properties

After-processing / in-service properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Service Temperature Range 10 to 160 °C -
Four-Ball Tester Wear Scar 0.9 mm Under 600 N load (DIN 51 350 pt.5)
Four-Ball Tester Weld Load 2,600 N DIN 51 350 pt.4
Almen Wieland OK Load 18,000 N -