MOLYKOTE 112

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE 112

Main features

  • Up to 232 deg C Service
  • Oil, Acid, and Alkali Resistance
  • Low-Volatility Joint Sealing

Product Description

MOLYKOTE® 112 High Consistency Valve Sealant is a stiff, nonmelting silicone grease used primarily as a robust valve lubricant and sealant. Formulated with polydimethyl silicone fluids and an inert amorphous silica filler, it is designed for demanding environments that require a high degree of mechanical stability. It maintains its consistency without carbonizing, melting, or hardening during prolonged exposure to elevated temperatures up to 232°C (450°F).

Key features

  • Extreme temperature stability: Serviceable from -40°C to 232°C (-40°F to 450°F) without melting, hardening, or carbonizing.
  • Harsh environment resistance: Highly resistant to water, most aqueous solutions of inorganic salts, dilute acids, alkalis, and many organic compounds.
  • Low volatility: Features very low vapor pressure, making it an excellent sealer for high vacuum or pressure systems.

Applications / Suitable for

  • Lubricating valves, O-rings, and plug-valves in chemical processing
  • Sealing synthetic rubber or plastic parts in vacuum and pressure systems
  • Lubricating mechanical devices like flow meters, fire extinguisher valves, and optical equipment

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Polydimethyl silicone fluids and silica filler - Silicone grease
Appearance White-translucent / off-white - Grease / Paste (CTM 0176)
Unworked Penetration 215 - -
Worked Penetration 230 - 60 strokes, maximum
Worked Penetration 240 - 100,000 strokes
Specific Gravity 1.1 - at 25°C (77°F) (CTM 0022)
Melting Point None - -
Flash Point > 101 °C Closed cup (> 214 °F)
Shelf Life 60 months From date of manufacture
Technical properties

After-processing / in-service properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Service Temperature Range -40 to 232 °C (-40 to 450 °F)
Bleed 0.03 % 24 hours at 200°C (392°F) (CTM 0033A)
Evaporation 0.8 % 24 hours at 200°C (392°F) (CTM 0033A)
Water Spray-Off 3.0 % ASTM D4049
Dielectric Constant 2.93 - at 100 Hz (CTM 0112)
Dielectric Constant 2.92 - at 100 kHz (CTM 0112)
Dissipation Factor < 0.0001 - at 100 Hz (CTM 0112)
Dissipation Factor < 0.004 - at 100 kHz (CTM 0112)
Dielectric Strength 490 volts/mil 50 mil gap (CTM 0114)
Volume Resistivity 2.9x10^15 ohm-cm at 23°C (73°F)
Arc Resistance 122 seconds CTM 0171