MOLYKOTE 106

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

MOLYKOTE 106

Main features

  • Heat-Curing Dry Film Lubricant
  • High-Load Coating Application
  • 70 to 250 deg C Service Range

Product Description

MOLYKOTE® 106 Anti-Friction Coating is a heat-curing, solvent-based dry film lubricant containing solid lubricants such as molybdenum disulfide and graphite dispersed in an organic binder. Formulated as a dark gray liquid, it cures to provide maintenance-free, permanent dry lubrication for metal-to-metal combinations. It is ideal for highly stressed friction combinations involving slow speeds or oscillating movements, especially where traditional oils and greases are unsuitable or where the risk of soiling must be avoided.

Key features

  • High load-carrying capacity: Withstands extreme contact pressures, exhibiting a Falex load capacity of 14,500 N on phosphatized surfaces.
  • Low coefficient of friction: Delivers excellent wear protection and low friction without the use of intentional polytetrafluoroethylene (PTFE) or per- and polyfluoroalkyl substances (PFAS).
  • Extreme temperature resistance: Maintains reliable dry lubrication across a broad service temperature range from -70°C to 250°C.

Applications / Suitable for

  • Dry lubrication of locks, hinges, joints, and magnetic armatures
  • Anti-seizure coating for engine and gear components
  • Highly stressed metal-to-metal friction combinations with low speeds or oscillating operation

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Chemical Composition Solid lubricants, organic binder, solvent - Contains molybdenum disulfide and graphite
Physical State / Appearance Dark gray - Liquid
Viscosity (Efflux Time) 37 s at 20°C (ISO4 cup, DIN EN ISO 2431)
Kinematic Viscosity > 20.5 mm²/s at 25°C (77°F)
Density 1.16 g/ml at 20°C (DIN 53217/2)
Flash Point 29.5 °C Closed cup (DIN ISO 2619) (85.1 °F)
Usable Life 36 months Stored between 0 and 40°C in unopened containers
Technical properties

After-processing / in-service properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Recommended Dry-Film Thickness 5 to 20 µm -
Curing Time 60 minutes at 150°C (object temperature)
Curing Time (Alternative) 30 minutes at 180°C (object temperature)
Service Temperature Range -70 to 250 °C -
Falex Load-Carrying Capacity 14,500 N Phosphatized surface
LFW-1 Wear (Rotating) 478 N Revolutions x 1,000 to µ=0.1 (F=2,860 N, n=72 rpm, v=7.9 m/min, phosphatized) (ASTM D2714)
LFW-1 Wear (Oscillating) 292 N Oscillations x 1,000 to µ=0.08 (F=900 N, frequency=89.5 osc./min, phosphatized) (ASTM D2714)