LORD 7550C Urethane Adhesive

Harmonization Code : 3907.30.00.15 | Epoxide resin, halogen-free

LORD 7550C Urethane Adhesive

Main features

  • Equal-Mix LORD 7550 Curative Component
  • 6,000 to 12,500 cP Viscosity
  • Lexan, ABS, and Primed-Metal Bonding

Product Description

LORD® 7550C Urethane Adhesive Curative is the curative component of the equal-mix LORD 7550 two-component clear urethane adhesive system. When combined 1:1 by volume with LORD 7550A resin, the system bonds Lexan, ABS, polycarbonate, other plastics, and properly prepared and primed metals. The clear-to-yellow liquid curative has a typical viscosity of 6,000 to 12,500 cP at 25°C. The mixed adhesive is self-leveling, has a typical working time of three to five minutes, reaches handling strength in approximately 60 minutes, and cures to full strength in about 72 hours at room temperature.

Key features

  • LORD 7550 curative component: LORD 7550C is mixed 1:1 by volume with LORD 7550A resin.
  • Controlled liquid viscosity: Typical component viscosity is 6,000 to 12,500 cP at 25°C.
  • Clear urethane bonding system: The paired system is documented for plastics and properly prepared and primed metals.

Applications / Suitable for

  • Curative component of the LORD 7550 urethane adhesive system
  • Bonding Lexan, ABS, polycarbonate, and other plastics
  • Bonding properly prepared and primed metals

Technical Specifications

General Properties
Appearance Appearance
Clear to Clear Yellow Liquid
Density Density
1078 -1126 kg/m3
Physical Properties
Viscosity Viscosity
6000 -12,500 mPa.s
Thermal Properties
Flash Point Flash Point
>93 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Component role Curative N/A LORD 7550C
Appearance Clear to clear-yellow liquid N/A As supplied
Viscosity 6,000 to 12,500 cP At 25°C
Density 1,078 to 1,126 kg/m³ As supplied
Flash point >93 °C Closed cup
Shelf life 6 months At 21°C to 27°C in the original unopened container

Leading Brands Trust in Our Products and Services