LORD 7545A/D

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

LORD 7545A/D

Main features

  • High-Strength Structural Bonding
  • Non-Sag Vertical Placement
  • Solvent and Weather Resistance

Product Description

Overview

LORD® 7545-A/D Urethane Adhesive is a two-component, equal-mix urethane adhesive system designed for bonding FRP, SMC, primed metals, and other plastics with minimal surface preparation. The adhesive system is formulated to bond dissimilar substrates while providing high strength and durable structural performance. The 7545 system is available with multiple curatives to accommodate different process requirements, with the 7545-A/D combination offering an intermediate working time. 

Key Features

  • Two-component 1:1 mix urethane adhesive system.
  • High-strength, durable structural bonding performance.
  • Bonds FRP, SMC, primed metals and various dissimilar substrates with minimal surface preparation.
  • Non-sag formulation for vertical and overhead applications.
  • Resists weathering, humidity, salt spray and solvents after cure.

Suitable For

  • Fiber reinforced plastic (FRP) assemblies
  • Sheet molding compound (SMC) assemblies
  • Primed metal bonding
  • Bonding dissimilar substrate combinations

Technical Specifications

No specifications available.

Additional Information

As-Supplied / Before-Processing Properties

Property 7545-A Resin 7545-D Curative
Appearance Brown paste Off-white or black paste
Viscosity (Brookfield, 25°C) 25,000–70,000 cP 230,000–650,000 cP
Density 12.5–12.8 lb/gal (1498–1534 kg/m³) 10.6–11.0 lb/gal (1270–1318 kg/m³)
Flash Point (Closed Cup) >200°F (>93°C) >200°F (>93°C)
Mix Ratio 1:1 by volume (1:0.85 by weight)
Solids Content 100 wt%
Working Time @ 75°F (24°C) 11–18 minutes
Time to Handling Strength @ 75°F (24°C) 90 minutes

After-Processing / Final-State Properties

Property Value
Hardness Shore D 67
Tensile Strength at Break (ASTM D882) 3000 psi (20.7 MPa)
Elongation (ASTM D882) 72%
Young's Modulus (ASTM D882) 22,200 psi (153 MPa)
Glass Transition Temperature, Tg (ASTM D3418) 116°F (47°C)
Moisture Absorption (ASTM D570) <1%

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers