LORD 410/19 GB

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LORD 410/19 GB 4:1 375ML

Main features

  • Acrylic Metal/Engineered-Plastic Structural Adhesive
  • 20 to 30-Minute Working Window
  • 18.6 MPa Cured Tensile Strength

Product Description

LORD® 410 Acrylic Adhesive is a two-component acrylic structural adhesive used with LORD Accelerator 17, 19, or 19GB to bond prepared or unprepared metals and engineered plastics. The non-sag adhesive component has a typical viscosity of 100,000 to 300,000 cP at 25°C. When mixed with a recommended accelerator, the LORD 410 system provides a typical working time of 20 to 30 minutes, handling strength in 60 to 120 minutes, and full cure in 24 hours at 24°C. Typical cured properties with Accelerator 19 include 18.6 MPa tensile strength and 30% elongation.

Key features

  • Multi-substrate structural bonding: The adhesive system is documented for metals and engineered plastics.
  • 20 to 30-minute working time: The mixed LORD 410 system provides handling strength in 60 to 120 minutes at 24°C.
  • Accelerator options: Accelerators 17, 19, and 19GB support different mix ratios and processing configurations.

Applications / Suitable for

  • Bonding prepared or unprepared metals
  • Bonding XENOY, polycarbonate, ABS, and acrylic plastics
  • Assemblies requiring impact and peel resistance

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Appearance Off-white to tan paste N/A LORD 410 adhesive component
Viscosity 100,000 to 300,000 cP Brookfield at 25°C
Density 1,096 to 1,156 kg/m³ As supplied
Working time 20 to 30 min Mixed with recommended accelerator at 24°C
Time to handling strength 60 to 120 min 50 psi shear at 24°C
Full cure 24 h At 24°C
Technical properties

After-processing / final-state properties

Typical final-state values under the stated system and test conditions. These values are not sales specifications.

Property Value Unit Method / condition
Tensile strength 18.6 MPa LORD 410 with Accelerator 19; ASTM D638 modified
Elongation 30 % LORD 410 with Accelerator 19; ASTM D638 modified
Young's modulus 896.3 MPa LORD 410 with Accelerator 19; ASTM D638 modified
Glass-transition temperature 72 °C LORD 410 with Accelerator 19; ASTM E1640-99 by DMA
Service temperature -40 to 149 °C Documented adhesive-system range