LOCTITE SICOMET 100

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE SICOMET 100

Main features

  • 0.01 to 0.50 mm Gap Fill
  • Fast Moisture-Cure Fixturing
  • Strong Rubber/Plastic Adhesion

Product Description

LOCTITE® SICOMET 100 is a fast-curing, medium-viscosity ethyl cyanoacrylate instant adhesive designed for bonding a wide range of materials including plastics, rubbers, metals, fabrics, and foam materials. The one-component adhesive cures rapidly through surface moisture and develops handling strength within seconds on close-fitting parts. It offers excellent adhesion to plastics and elastomers while requiring no mixing, making it suitable for high-speed assembly and repair operations.

Key Features & Benefits

  • Ethyl cyanoacrylate instant adhesive technology.
  • Excellent adhesion to rubbers and plastics.
  • Fast fixture and cure speed.
  • Medium-low viscosity for easy application.
  • One-component formulation requiring no mixing.
  • Easy dispensing and handling.
  • Suitable for close-fitting assemblies.

Recommended Applications

  • Plastic component assembly.
  • Rubber and elastomer bonding.
  • Foam material bonding.
  • Metal bonding applications.
  • Fabric assembly and repair.
  • General-purpose instant bonding operations.
Product Family

LOCTITE SICOMET 100

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance Appearance
Colorless liquid
Specific Gravity Specific Gravity
1.05 - 1.10
Physical Properties
Viscosity Viscosity
140 - 220 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Ethyl Cyanoacrylate — Instant adhesive
Appearance Colourless Liquid — Uncured material
Components One Part — No mixing required
Viscosity Classification Medium-Low — Product characteristic
Specific Gravity 1.05 - 1.10 — 25°C
Viscosity 140 - 220 mPa·s (cP) 25°C
Cure Mechanism Surface Moisture — Moisture activated
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Recommended Gap Fill 0.01 - 0.50 mm Typical bond gap
Fixture Time (Aluminium) 5 - 10 seconds Typical cure speed
Fixture Time (Steel) 10 - 30 seconds Typical cure speed
Fixture Time (Rubber, Nitrile) 5 - 10 seconds Typical cure speed
Fixture Time (ABS) 5 - 10 seconds Typical cure speed
Fixture Time (PVC) 5 - 10 seconds Typical cure speed
Tensile Shear Strength (Steel) 17 N/mm² ISO 4587, 24 h cure
Tensile Shear Strength (Aluminum) 15 N/mm² ISO 4587, 24 h cure
Tensile Shear Strength (ABS) 8* N/mm² Substrate failure