LOCTITE SI 5040

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

LOCTITE SI 5040

Main features

  • One-Component Sealing System
  • Non-Corrosive Sealing Formulation
  • Self-Leveling Flowable Placement

Product Description

LOCTITE® SI 5040™ is a one-component alkoxy silicone RTV sealant designed for potting, coating, and sealing automotive, electronic, military, and industrial components. The self-leveling, non-corrosive formulation provides uniform cavity filling while maintaining flexibility, shock absorption, and environmental durability. After curing, it forms a resilient silicone elastomer that resists moisture, ozone, weathering, and harsh service environments while maintaining performance at temperatures up to 200°C.

Key Features & Benefits

  • One-component RTV alkoxy silicone system.
  • Non-corrosive curing mechanism.
  • Self-leveling for uniform cavity fill.
  • Excellent moisture, ozone and weather resistance.
  • Provides flexibility and shock absorption.
  • Suitable for potting, coating and sealing applications.
  • Tested to MIL-A-46146B requirements.

Recommended Applications

  • Electronic component potting.
  • Protective conformal coating.
  • Industrial sealing applications.
  • Automotive component protection.
  • Military and environmental sealing systems.
Product Family

LOCTITE SI 5040

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance Appearance
Translucent milky white viscous liquid
Specific Gravity Specific Gravity
1.05
Physical Properties
Viscosity Viscosity
85,000 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Silicone — RTV sealing and potting compound
Chemical Type Alkoxy Silicone — Non-corrosive system
Appearance Translucent Milky White Viscous Liquid — Uncured material
Specific Gravity 1.05 — 25°C
Solids Content ≥92 % Non-volatile content
Viscosity 85,000 mPa·s (cP) Brookfield RVT, spindle 6, 2.5 rpm
Viscosity 35,000 mPa·s (cP) Brookfield RVT, spindle 6, 20 rpm
Storage Requirement 2 to 8 °C Recommended storage range
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Maximum Service Temperature 200 °C Typical operating limit
Shore Hardness ≥15 Shore A ISO 868
Elongation at Break ≥150 % ISO 37
Tensile Strength ≥1.0 N/mm² ISO 37
Tear Strength 17.5 N/mm ISO 34-1 Die B
Water Absorption 0.05 % 24 h @ 23°C
Dielectric Breakdown Strength 16 kV/mm IEC 60243-1
Volume Resistivity 7 × 10¹⁶ Ω·cm IEC 60093
Lap Shear Strength (Steel to Glass) 1.8 N/mm² 1 week cure @ 23°C
Lap Shear Strength (Glass to Glass) 1.7 N/mm² 1 week cure @ 23°C